Just a quick question, I was trying to have a play with the Iris Gold and Straw Yellow Faux Boro today and there are colours in there but it's all very dark. What have a I done wrong and can anybody show me what it should look like, I was expecting something brighter.
Thanks
Julia
http://www.frit-happens.co.uk/forum/index.php?topic=24002.0
and there are some more in the recipes section too!
Kazx
If you are getting a dark cola colour to the bead then you have a duff batch of Straw Yellow. Don't waste any more of your time with it. Try a different supplier. But beware - these suppliers don't half get bolshy if you tell them their straw yellow is rubbish...... ;)
you have to encase it! i didn't know this when i first started and wondered why it was really hard to see the colours ;)
It should look like this - and ys, it does look better if you encase it but if you aren't getting any colours to begin with then it probably is the Straw Yellow.
If it's not the Straw Yellow then DON'T be tempted to reduce it - it's just a colour reaction which occurs in a NEUTRAL flame.
(http://farm5.static.flickr.com/4002/4294099652_42ef5bcc4f.jpg) (http://www.flickr.com/photos/31197390@N08/4294099652/)
Rainbowdrops2 (http://www.flickr.com/photos/31197390@N08/4294099652/) by redhotsalbeads (http://www.flickr.com/people/31197390@N08/), on Flickr
I did try encasing it! But you're right Sal the yellow has turned a cola colour behind the colours, they are there it's just too dark. Fortunately I didn't buy much. Oh well, maybe I'll add it to my shopping list for Flame Off, how frustrating! :(
Julia
Quote from: Redhotsal on March 08, 2011, 09:13:53 PM
If you are getting a dark cola colour to the bead then you have a duff batch of Straw Yellow. Don't waste any more of your time with it. Try a different supplier. But beware - these suppliers don't half get bolshy if you tell them their straw yellow is rubbish...... ;)
I imagine the manufacturer is at fault. I doubt the supplier can test every batch that comes through the door - we'd all be expecting second hand prices on used rods :D
Also the base colour can make a difference, for example if you wind your iris/straw mix onto dark ivory then the reaction will make it kinda dark and lacking the colours you see in Sal's (amazing!) beads.
(http://farm5.static.flickr.com/4121/4739302825_f11fee2f55_m.jpg) (http://www.flickr.com/photos/51048389@N02/4739302825/)
S6301231 (http://www.flickr.com/photos/51048389@N02/4739302825/) by Avalon Beads (http://www.flickr.com/people/51048389@N02/), on Flickr
This was my attemp, but as Sal said I did go though a batch of poo until I changed my straw yellow.
If your straw yellow is duff, there are some other colours that give the same effect. 073 pale green apple works, and I think 090 kelp and 068 pale rose are supposed to as well (haven't tested those myself yet). Melanie Graham's found some other ones too on her blog, but I can't remember what they were! Maybe CiM mojito?
Light trans brown and some of the ambers work - but the best colours are to be had from Straw Yellow.