Frit-Happens !

Lampwork => Common Problems => Topic started by: Sarah A on February 25, 2011, 05:11:49 PM

Title: Help with beads please
Post by: Sarah A on February 25, 2011, 05:11:49 PM
Hi really hoping some of you lovely people can help me.  I have been trying to make beads that are the same or similar size and wondered if anyone had some hints and tips they could give me.

I am also saving to buy some new tools etc and just wondered what people would recommend.  At the moment I only have what came with my kit so it's a rake, tweezers and graphite paddle.  Would really like some other tools but don't have lots to spend so if anyone has something they recommend someone new to buy to help them that would be great. 

Thanks Sarah
Title: Re: Help with beads please
Post by: helbels on February 25, 2011, 05:19:02 PM
Hi Sarah

If you want to make consistently sized beads very easily then I can't recommend better than a round beadroller from CGBeads - they make it so easy - yes, you can keep practicing, but in the meantime, these gadgets make consistent bead sizes a certainty.
Title: Re: Help with beads please
Post by: ScarletLeonard on February 25, 2011, 05:38:42 PM
Beat me to it Helen, Yes a bead roller is a great way to make consistant sizes
there's also some here.
http://www.frit-happens.co.uk/forum/index.php?topic=26938.0;topicseen
from a German bloke, (later in the thread there is a link to a translated version of the ebay store.) they are brass and not graphite but the reviews seem to be very good and the price is nice.

There's loads of different methods
I started making pairs on one mandrel (lots of ppp there and the increased chance of casualties.) to get them as close in size as possible.
You can also make up blank beads to hold up and check the size of the one you are making
There are also some 'bead callipers' which are a large loop made of stainless steal to help you measure.
Some people measure and mark rods of glass
Some mark the mandrel
Some count how many wraps of glass they have put on.

Some people are just plain lucky and can easily gauge by eye.

One thing that is worth remembering hot glass looks bigger than cool glass, so even if you make and anneal the first one then use that as a gauge you will end up with a difference.

In the end it all comes down to what works for you, you may find that none of these work and come up with your own method.
Title: Re: Help with beads please
Post by: TheJanie on February 25, 2011, 05:41:51 PM
When I first started making beads, I printed a number of different-sized oval silhouettes on one sheet of paper and put it somewhere handy (but obviously not too close to the flame)!

I made my first bead, decided which silhouette it was closest to in size and then used that with the rest of the beads in that session.  With each subsequent bead I started really small and added glass until it closely matched the relevant size.

There are probably better ways to do it but it worked for me :)
Title: Re: Help with beads please
Post by: Clair on February 25, 2011, 05:45:31 PM
It is just down to practice (always the way!) but one hint I picked up from a very good friend of mine was to pre-mark her torch top marver with sizes of beads (9/10/11/12 mm etc) That way she could measure the size of the bead exactly. Good luck.x
Title: Re: Help with beads please
Post by: noora on February 25, 2011, 05:56:17 PM
About the tools, you can find some tools in your kitchen, for example a spoon and a table knife that you can use for shaping and poking. The spoon is also useful for holding frits and powders. Just dip them in a jar of water to keep them cool so that the glass won't stick. I also used a thin steel knitting needle for poking until I accidentally left it in the water jar too long so that it got rusty (obviously it wasn't stainless steel...). Then I bought a set of soldering picks from the hardware store, and they've been great (like this (http://www.tickintimeworldofwatchtools.co.uk/soldering-aid-tools-6-pc-set-points-scrapers-picks-and-brushes-1049-p.asp), but I bought them from a local store, not online).

What tools you need depends on what you want to do. I'm still a newbie myself so I can't really recommend :) I've been quite happy so far with my various poking and shaping tools, and the tweezers, soldering picks and graphite paddle are the tools I use the most. The next thing I want to buy is a a lentil press and perhaps a bead roller.
Title: Re: Help with beads please
Post by: Katiequiggle on February 25, 2011, 07:40:56 PM
I agree with Noora, there are lots of things in your kitchen drawer you can use.  For a long time I used to use my pallette knife from the kitchen instead of a marver which worked fine.  I'd be using it still if I hadn't been given a marver for my birthday.  A veg knife is really handy and long tweezers are useful too.  One of my brought tools which I use a lot is a masher, a nice wide one that closes together without making the bead thicker one end and thinner the other.
Title: Re: Help with beads please
Post by: Sarah A on February 26, 2011, 06:10:09 PM
Brilliant thanks so much everyone for your helpful comments. I am going to try some of the tips for getting beads the same size whilst waiting for a beadroller and mashers sound good too.  Thanks again this really has helped.
Title: Re: Help with beads please
Post by: Purple Cobwebs on February 27, 2011, 06:29:58 PM
Quick question on the beadroller.....how do you stop your bead release flaking off the mandrel and fouling te bead when you're spinning the bead in the roller?
I've had this problem with presses. Or am I just too heavy handed?!!! ???
Title: Re: Help with beads please
Post by: sarah t on February 27, 2011, 08:50:05 PM
bead realease falling off is a problem for me too using any press but less with the rollers ......for me its tapping /flicking with tweezers the bits off and a paint brush ....i always brush out the press between pressing

Title: Re: Help with beads please
Post by: Clair on February 27, 2011, 08:59:45 PM
I'm not an expert on presses and have never used a bead roller but I was told to be quite gentle when using a press. I was also told not to have the glass too molten, but I don't know whether that has any bearing on the bead release. I always try and press gently over the centre of the bead, so the press doesn't come into contact with the mandrel (and therefore the bead release)
Title: Re: Help with beads please
Post by: ♥♥Tan♥♥ on February 27, 2011, 09:04:20 PM
If the release starts to flake I have a pair of needle nose pliers that I use to eat away the release from either side of the bead so its just bare mandrel touching the press.
Title: Re: Help with beads please
Post by: Purple Cobwebs on February 27, 2011, 10:33:05 PM
Thanks for the tips. Very tempted to invest in a bead roller or two now!!!!! :)