Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: laurat on February 25, 2011, 12:19:15 PM

Title: Slumping question
Post by: laurat on February 25, 2011, 12:19:15 PM
Hi

i tried to slump a panel this week and it didn't quite work.

I used float glass and it did go the right shape but the edges were all wavey, not in an attractive way either just all over the place. and the edges of some of the coloured glass was a little bit crinkley and i had sharp edges that were not there before.

I am very disappointed as I really liked the desgin but now it looks a bit of a mess.

I know that it could be due to the high temp, but I am never quite sure which bit of the firin to change, the ramp rate ot the top temp? I don't have photos or the schedual with me as I am at work but I am sure that the top temp is 537C.

Many thanks

laura
Title: Re: Slumping question
Post by: Zeldazog on February 25, 2011, 12:33:43 PM
It would be more helpful if you could post the schedule, and of course a photograph, it might help us understand a bit more.

537 sounds more like the start of the annealing zone to me...

When you want to alter a process (i.e. you want to slump rather than fuse) you need to alter the process temperature - the rate is important, as the more you fire something, and the thicker it is, and the bigger it is, the slower you have to go, but rate is pretty much irrelevant if you over fire something.
Title: Re: Slumping question
Post by: laurat on February 28, 2011, 12:12:47 PM
Right the firing was

Inital Heat 538c/hr to 538c 0.00 hold

rapid heat process soak afap to 824c 0.20 hold

rapid cool anneal soak afap to 538c 0.15 hold

anneal cool 182c/hr to 427c 0.00

cool to room temp afap to 25c


I am struggling to get the photo onto this laptop as it is a bit wonky.

but all adice is very welcome.

laura
Title: Re: Slumping question
Post by: Zeldazog on February 28, 2011, 03:27:32 PM
Yikes!!

Please have a good read of the Bullseye tech-notes before you do anything else.  See here:  BULLSEYE TECHNOTES (http://www.bullseyeglass.com/education/#techbook) - The Heat & Glass #4 is particularly helpful as a starting point.

I know you're working in float, but if you take a look through some of these, you'll see your firing schedules are way out.  I generally full fuse my float about 30 to 35c degrees hotter, and slump about 20 degrees hotter than my normal Bullseye schedules.


I'd say no need for the photograph in all honesty, it's definitely been fired too hot.
Title: Re: Slumping question
Post by: laurat on February 28, 2011, 04:05:19 PM
Thanks for your advice

I will have a look and see what changes I can make.

I will report back and let you now how I get on.

Laura
Title: Re: Slumping question
Post by: ♥♥Tan♥♥ on March 02, 2011, 04:34:08 PM
What thickness of glass are you firing?
Title: Re: Slumping question
Post by: Flyingcheesetoastie on March 02, 2011, 09:05:31 PM
Another thing i've picked up on in your first post is the two different glasses, you mention float and 'coloured glass', is this float compatible or are you introducing further problems by using different glass that isn't compatible?

Hope that makes sense, compatability is a major factor in any kind of glass melting.
Title: Re: Slumping question
Post by: laurat on March 02, 2011, 10:27:00 PM
Hi

Its a sheet of 3mm clear float glass with compatable coloured glass on the top.

I have slumped a 3 mm sheet of bullseye glass with randomly placed bullseye glass on it, this time it did stay in better shape but it seems that there was air trapped between the glass and the mould. I check the air holes in the mould and these were clear. Itlooks like the temperature didnt reach the same high as the other side. I was thinking that i may try and slump it again.The annoying thing is I really like the design!

Thanks for all the help, I really appreciate it. I have the ideas but the firing side is leaving me stumped!!
Title: Re: Slumping question
Post by: Flyingcheesetoastie on March 02, 2011, 10:41:38 PM
So you used the programme devised for float glass on a bullseye glass firing?  Or you did a different firing with the bullseye glass?

It sounds like your learning loads by trying different things out and getting unique results, which is the best way to learn!

Keep at it and we'd love to see pictures of your creations too!
Title: Re: Slumping question
Post by: laurat on March 02, 2011, 11:14:47 PM
I used a different schedule for the bullseye - I learnt very quickly that different glass needs different temps!

I have kept a good record of what I have done and taken lots of notice of things said on the threads here.

How often can i reheat and mould the glass?

I amgoing to take a load of photos next week and have a go at flicker too.
Title: Re: Slumping question
Post by: laurat on March 17, 2011, 10:16:37 PM
I have done it!!!

Thanks to all your advice I have what I consider to be an amazing dishy!

(http://farm6.static.flickr.com/5097/5535188961_97257f02c1_m.jpg) (http://www.flickr.com/photos/60629001@N08/5535188961/)
Cherry Dish (http://www.flickr.com/photos/60629001@N08/5535188961/) by lilacstars (http://www.flickr.com/people/60629001@N08/), on Flickr
Title: Re: Slumping question
Post by: Aurorabelfast on March 22, 2011, 09:31:02 PM
Love it!!
Title: Re: Slumping question
Post by: laurat on March 22, 2011, 10:08:11 PM
I have a poppy one to slump this week. ;D

Its addictive!
Title: Re: Slumping question
Post by: Les on March 22, 2011, 10:09:44 PM
Brilliant ! I love poppies ... I even named my daughter after them ;D
Title: Re: Slumping question
Post by: Pat from Canvey on March 23, 2011, 09:01:03 AM
Well done. I love poppies too, lets see the pictures.
Title: Re: Slumping question
Post by: laurat on March 23, 2011, 02:26:42 PM
I am hoing to add a photo in the next couple of days, it is in the kiln as I type this so i ma super excited, I have sunflowers to do next.  ;D

I have a fair and I am hoping to sell out!!! I know I can dream!!  ::)
Title: Re: Slumping question
Post by: ♥♥Tan♥♥ on March 23, 2011, 03:40:59 PM
Those cherries are fab, is that the fully fired article now? Did you sort out the sharp edges?
Title: Re: Slumping question
Post by: laurat on March 23, 2011, 04:55:59 PM
yes it is finished, the shape edges didn't happen this time, there is a bit of a rough corner, but i have a buffer that sorted this out.

It doesn't really show the curve of the glass, I was so pleased with it as I had the two disaters before, even tho my mum has said to take one of them with me to my next fair!

Laura
Title: Re: Slumping question
Post by: ♥♥Tan♥♥ on March 23, 2011, 05:21:00 PM
I bet you are so pleased to have targeted the problems and be able to create something you are really happy with. More pics now ;)