Does anybody know what type of filters we are supposed to use for protection against metal fumes and enamels? Is P1, P2 or P3?
I was told a few days ago and I can't remember now ???

Thank you

Annelyse
Title: Re: Respiratory protection
Post by: Buzzybead on June 18, 2007, 06:15:29 PM
P3!! Apparently B&Q make a really good mask with changeable filters for about £35.00. MUCH better than the disposables I bought.
Title: Re: Respiratory protection
Post by: Caroline on June 18, 2007, 06:19:59 PM
they don't at the B&Q in Aberdeen! I've already checked!
Title: Re: Respiratory protection
Post by: Buzzybead on June 18, 2007, 07:29:59 PM
Hmm: this is dear but wouls stop a nuclear attack!

http://www.screwfix.com/app/sfd/cat/pro.jsp?cId=A331070&ts=91275&id=14060
Title: Re: Respiratory protection
Post by: Buzzybead on June 18, 2007, 07:34:18 PM
Or this?

http://www.sevsafe.co.uk/acatalog/3M_Half_Mask_Respirators.html
Title: Re: Respiratory protection
Post by: Annelyse on June 18, 2007, 08:00:26 PM
Thanks for the reply! How could I not remember ...It must be all the lead getting to my brain... :-[ ;)

I looked at both B&Q in Aberdeen and no...nothing :(