Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: Zeldazog on February 18, 2011, 03:40:53 PM

Title: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Zeldazog on February 18, 2011, 03:40:53 PM
I made a beautiful red fused and slumped dish a few weeks ago but was struggling to remove patches of kiln wash from the reverse.

I'd even tackled it with a diamond hand pad, now got a lovely satin finish on the back  ;D ;D - but still left me with a few little patches of batt wash that I couldn't get to.

I remembered reading about Cillit Bang for beads, so I got a bottle and gave it ago - MIRACLE!  I've scrubbing at this dish for ages.... now I know better (and I will be trying it on those three beads me and Ashley made that are still stuck on the mandrels!)

Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: ScarletLeonard on February 18, 2011, 07:26:16 PM
I've not heard the cillit bang tip.

does it do a good job on removing bead release?

Good news for your dish though even if you had to learn the hard way :)
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Zeldazog on February 18, 2011, 08:21:58 PM
Quote from: ScarletLeonard on February 18, 2011, 07:26:16 PM


does it do a good job on removing bead release?



I recall reading on here that it was good for getting stuck beads of mandrels, and also for removing grey scum from turquoise beads?
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: ♥♥Tan♥♥ on February 18, 2011, 08:37:35 PM
Don't you love it when a plan comes together
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: shaz on February 18, 2011, 08:46:14 PM
Ohh good just got from tesco at buy 1 get 1 free ;D
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Zeldazog on February 18, 2011, 09:08:19 PM
It is the Lime & Grime one that does the trick, isn't it?  Well, that's the one I bought and it seems to have worked...

Mind you, I do wonder exactly what unhealthy things are in it - the fact that it can shift twice fired on batt wash, that wouldn't come off with wire wool or a green pan scrubber, after soaking in soapy water for days - but a few minutes of this and well, bang and the batt wash is gone!  I dread to think what nasties are in it really (not something I will be using at home on the work surfaces!)
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Hamilton Taylor on February 19, 2011, 01:56:31 PM
We use it for all sorts of cleaning and degreasing, I've no idea what's in it, but it doesn't half sting in a cut!
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Blue Box Studio on February 19, 2011, 02:26:08 PM
It's great for most things but I can't get it to work on the grey stuff on turquoise beads.  Should I be soaking?  I left sitting in Grime and Lime for an hour but didn't work - so is the loo cleaner Grime and Lime the right stuff, or the kitchen spray?  I didn't know there was so much to choose from until I told DH to get me Grime and Lime and he came back with rather a lot of cleaner for one little bead.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Pat from Canvey on February 19, 2011, 04:06:59 PM
Quote from: Zeldazog on February 18, 2011, 09:08:19 PM
It is the Lime & Grime one that does the trick, isn't it?  Well, that's the one I bought and it seems to have worked...

Mind you, I do wonder exactly what unhealthy things are in it - the fact that it can shift twice fired on batt wash, that wouldn't come off with wire wool or a green pan scrubber, after soaking in soapy water for days - but a few minutes of this and well, bang and the batt wash is gone!  I dread to think what nasties are in it really (not something I will be using at home on the work surfaces!)
It probably has an acid base, but what's the worry about acids. You put vinegar (acetic acid) on chips and citric acid (lemon juice ) on pancakes and oh yes you have hydrochloric acid in your stomach to help digest food. (Think about acid reflux and the chalky i.e. alkali pills you take to combat it. It's the strength of the acids you should worry about. Rhubarb has oxalic acid in it that's why we don't eat the leaves.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Zeldazog on February 19, 2011, 04:29:43 PM
Quote from: Pat from Canvey on February 19, 2011, 04:06:59 PM
. It's the strength of the acids you should worry about. Rhubarb has oxalic acid in it that's why we don't eat the leaves.

I think that's the point Pat - my dish was soaked in acetic acid (or should I say white vinegar) over night and nothing. 2 minutes in cilit bang....
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: ♥♥Tan♥♥ on February 19, 2011, 04:35:48 PM
I have to say, imagine a house that hasn't been touched for two years, the toilet left uncleaned and the kitchen had food fried in it every day, plus, two heavy smokers.........................Cillit bang shifted it.

Stinks like a bugger, stings like a bugger but it does the job.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: ★★Terri★★ on February 19, 2011, 04:45:16 PM
Quote from: Blue Box Studio on February 19, 2011, 02:26:08 PM
It's great for most things but I can't get it to work on the grey stuff on turquoise beads.  Should I be soaking?  I left sitting in Grime and Lime for an hour but didn't work - so is the loo cleaner Grime and Lime the right stuff, or the kitchen spray?  I didn't know there was so much to choose from until I told DH to get me Grime and Lime and he came back with rather a lot of cleaner for one little bead.

Sue I soaked a couple of copper green beads that had loads of grey stuff on them overnight and almost all of it went.  I have been using the bathroom grime and lime spray - just sprayed loads of it into a small jam jar, giving it a bit of time to let the froth settle down.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Blue Box Studio on February 19, 2011, 05:08:48 PM
Quote from: Terri on February 19, 2011, 04:45:16 PM
Sue I soaked a couple of copper green beads that had loads of grey stuff on them overnight and almost all of it went.  I have been using the bathroom grime and lime spray - just sprayed loads of it into a small jam jar, giving it a bit of time to let the froth settle down.

Right, will have another go then. Thanks.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Zeldazog on February 19, 2011, 05:11:35 PM
Quote from: Tan on February 19, 2011, 04:35:48 PM
I have to say, imagine a house that hasn't been touched for two years, the toilet left uncleaned and the kitchen had food fried in it every day, plus, two heavy smokers.........................

Ew.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: ♥♥Tan♥♥ on February 19, 2011, 05:50:32 PM
Worse than ew, more like..........oik oik oik erk :P
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Blue Box Studio on February 19, 2011, 06:26:27 PM
Quote from: Zeldazog on February 19, 2011, 05:11:35 PM
Quote from: Tan on February 19, 2011, 04:35:48 PM
I have to say, imagine a house that hasn't been touched for two years, the toilet left uncleaned and the kitchen had food fried in it every day, plus, two heavy smokers.........................

Ew.

Sounds just like a few of the  wards at Southmead hospital; the last one I was in the toilets stank, the shower was gross and plenty of original grime and lime round the sanitary ware.  Apparently it was a closed ward opened because they needed more bed space.  Ew sums it up quite well.  Seems only cleaners can clean toilet floors after old biddies wee everywhere (most inmates were in their dotage) and the one cleaner only came in once a day. G-r-o-s-s.  In fairness the first ward was better, no one was well enough to use the spotless bathroom, except wobbly me; but I was sleeping on a gurney in a store room.
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Scubeadoo on February 25, 2011, 09:28:47 PM
Quote from: Blue Box Studio on February 19, 2011, 02:26:08 PM
It's great for most things but I can't get it to work on the grey stuff on turquoise beads.  Should I be soaking?  I left sitting in Grime and Lime for an hour but didn't work - so is the loo cleaner Grime and Lime the right stuff, or the kitchen spray?  I didn't know there was so much to choose from until I told DH to get me Grime and Lime and he came back with rather a lot of cleaner for one little bead.

I find a quick soak in silver dip normally shifts that
Title: Re: The Wonders of Time Machine Fuel (or Cillit Bang as otherwise known)
Post by: Blue Box Studio on February 25, 2011, 11:10:52 PM
Really? I have some of that in the back of the cupboard, saw it this evening when I was looking for a spare fuse (and failed). Will re-rescue from my craft fair box and try again tomorrow.