I have a plan for a set, and I'm trying to put my finger on a really fresh mint green colour in the 104 palette. Cant think of one!! Copper green is close but too reactive, so is dirty martini but too creamy. Any suggestions?
Thanks! x
Green tea?
Kryptonite ?
Pea green?
Or if you are going for transparent have you thought about layering them?
I was going to also suggest Kryptonite or Peacock but I think you might find them to icy
(cross posts)
Kryptonite base with Mojito over the top?
this is kryptonite etched ...
(http://farm5.static.flickr.com/4120/5394882733_c3425c8bf7_m.jpg) (http://www.flickr.com/photos/urbanbeads/5394882733/)
kryptohearts (http://www.flickr.com/photos/urbanbeads/5394882733/) by Mad Cat Glass (http://www.flickr.com/people/urbanbeads/), on Flickr
nom nom colour!
les they are stunning!! I'll give it shot tomorrow but I was thinking something softer...aaaaarg, you know when you have an image in your head and you cant explain?! lol, I'll see if i can find the pantone! thanks guys x
it is a rather gorgeous colour isn't it :) it's slightly translucent if left unetched, but it's still lovely :)
Quote from: Jolene on February 16, 2011, 07:55:16 PM
nom nom colour!
I quite agree!
Effetre pale Emerald (031) is transparent but very similar in colour to copper green...
(http://farm2.static.flickr.com/1229/5120073779_04091af630.jpg) (http://www.flickr.com/photos/kays-beads/5120073779/)
Berry mint (http://www.flickr.com/photos/kays-beads/5120073779/) by Kays Beads (http://www.flickr.com/people/kays-beads/), on Flickr
These are Kryptonite unique, its slightly darker
Kryptonite is gorgeous, isn't it ;D .... I can't believe that I had a rod or two sitting in the bottom of my stash draw for ages too !
I love it with purple, makes the colour really 'pop'
(http://farm6.static.flickr.com/5255/5451161567_e873c93b67.jpg) (http://www.flickr.com/photos/helenfchalmers/5451161567/)
Mint Green? (http://www.flickr.com/photos/helenfchalmers/5451161567/) by helenfchalmers (http://www.flickr.com/people/helenfchalmers/), on Flickr
This is what I was thinking. Would prefer an opaque, or transluscent. hmmmm. Love those aswell Kay, so pretty x
Must buy some more !
Quote from: helenfc on February 16, 2011, 08:05:53 PM
(http://farm6.static.flickr.com/5255/5451161567_e873c93b67.jpg) (http://www.flickr.com/photos/helenfchalmers/5451161567/)
Mint Green? (http://www.flickr.com/photos/helenfchalmers/5451161567/) by helenfchalmers (http://www.flickr.com/people/helenfchalmers/), on Flickr
This is what I was thinking. Would prefer an opaque, or transluscent. hmmmm. Love those aswell Kay, so pretty x
The closest I remember to finding that colour was a bullseye colour that looked a bit like Jade ... not a 104 though I'm afraid
Sadly, the only thing I have resembling that colour is P & T :( Which is pretty much exactly the right shade.
bum. I had an inkling that would be the answer :( ;)
LE archive suggests CiM celadon or Eff Grasshpper?
http://www.lampworketc.com/forums/archive/index.php/t-61942.html
I have some Celadon, but it looks a bit dark ... never tried grasshopper though
I have no spare Kryptonite, but I have a part rod of Celadon if you just need a bit to try before you buy ?
Thanks Les, I have a rod of celadon lying around from a CIM mixed pack, it does look a bit dark I'm thinking grasshopper may be the way forward, off to have a rootle to see if i have a random rod of it! :)
Thanks for the link Vicki! :-*
Most welcome, hope you find something! xx
How about Elephaba?
Quote from: Cecilia on February 16, 2011, 08:24:32 PM
How about Elephaba?
Love this colour! It's a bit like the lime part of a chocolate lime, YUM! ;D
I think grasshopper may be a bit strong - I would go for green tea.
It's the base on these
(http://farm5.static.flickr.com/4130/5188847823_5edf29983d.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5188847823/)
Commission - Jan (http://www.flickr.com/photos/cheekycherubdesigns/5188847823/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Green Tea is definately Mint Green - its yum !
I love tea green, but the batches can vary a bit.
Might the answer to your question lie here?
http://www.serenasbeadery.com/color%20gallery.asp
I have just posted a picture of all the greens I have that could possibly be considered mint. (sorry I haven't figured out how to post directly from phone to here)
http://www.facebook.com/album.php?aid=266001&id=569680027&l=0f4f0ddd7b
(hope that works)
I reckon you should try the pale emerald green over a core of white and etched. I've put the part numbers of all the colours I've got on there too
Grasshopper?
The little spacer of grasshopper I've made looks a good match to that shade on my monitor. Your monitor may vary :D
I have some green tea, my batch seems a lot more white than what you have Kaz (they are so pretty!) I agree the grasshopper is too green green. (if you know what i mean!)
Sabine that website looks awesome, her copper green is exactly what I'm looking for!! Mine is like the dirty copper green though. :(
And Krysia, I love your spacer organisation!! need to see if I have any pale emerald!
xx
Reichenbach do one called mint green in 104 the same colour as you posted
Ionly have 1/2 rod other wise you would be very welcome to it
I am sure I got it from Martin if not it was Plowdens
Is it definitely 104? Reichenbach's website has a mint green in 96 but not 104.
Sure it was 104 I only had one rod and would love some more