Does anyone have any tips on how to encase beads on a hothead?! I always do too much and end up with big hulking ugly, UNSHAPABLE mammoth beads with totally distorted designs. I don't have any presses or special marvers so it's all hand-formed or whatever and it's impossible :P

How cold does the bead have to be before encasing/do you start with a big ass blob and do stripes or what? :P I kinda made another clear bead over the base bead...if that makes sense- as if the original bead was part of a really big mandrel :P But it DOESN'T work people and you lose all your work :P

Help please! :( Thanks, Dean ;D x
Title: Re: Encasing! ...or lack thereof
Post by: sparrow on February 16, 2011, 06:59:49 AM
Hi Dean, have you tried pulling a clear rod into stringer and using that to spiral-encase? You can use a rake or dental tool to gently pull the encasing towards the holes.
Title: Re: Encasing! ...or lack thereof
Post by: SilverGems89 on February 16, 2011, 07:13:01 AM
yep i agree with Sabine, try using stringer to encase! there are many techniques though, you can do stripes, continuous spiral, and even dots! have a look around online and i'm sure you'll find a few tips and tricks and at the end of the day its all about experimenting and finding what works for you!

ETA: i wish effetre made 006 commercial stringer, i'd buy it by the truck load (my stringer pulling skills are not all that!)
Title: Re: Encasing! ...or lack thereof
Post by: Kaz on February 16, 2011, 07:46:54 AM
It can be done Dean - just need PPP!
I made these on a hothead in Oz a couple of years ago
(http://farm4.static.flickr.com/3180/2953524745_183c7ed305.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/2953524745/)
Copy of IMG_7043 (http://www.flickr.com/photos/cheekycherubdesigns/2953524745/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
You need a small base bead and if poss marver it slightly into a small cylinder. Then keep it behind the flame so it stays solid but keeps warm and then heat the encasing glass to very gloopy and wind on as you describe, making sure you press enough to keep out any bubbles, but not so much that you break the bead release!
Kazx
Title: Re: Encasing! ...or lack thereof
Post by: princess pink on February 16, 2011, 08:09:48 AM
Hey Dean, I always struggled with encasing too! Have a look at Laura sparling's free tutorial on thin and thick encasing! It really works and this is how I do it.

http://www.beadsbylaura.co.uk/BBLDownloads.htm
Title: Re: Encasing! ...or lack thereof
Post by: ★★Terri★★ on February 16, 2011, 04:21:56 PM
Hi Dean - I use a hot head as well - so I sympathise.  I have been struggling with encasing for ages - and then I gave in a bought a tutorial and I am improving a lot.  Not perfect yet - but getting there.

I got Mary Lockwoods Encasing Boot Camp - http://www.etsy.com/listing/66937338/24-hour-sale-encasing-bootcamp-tutorial  - it's currently just over £6.  There are loads of clear step by step photos - various techniques, hot and handy tips and even a link or two to some video demos.  Well worth the money IMHO.

I have also been using some Laucsha clear that I got from Ray Skene on Ebay (he is a forum member) that is well suited to hot heads can't remember exactly what it's called - something like 'reformulated' but it melts nice and easy - is big chunky rods which you can use neat - or pull into stringers if you prefer. ;D  I have also tried Reichebach clear and Effetre clear - but they, like so many clear glasses, are a bit stiff.
Title: Re: Encasing! ...or lack thereof
Post by: MyPrecious on February 16, 2011, 04:46:39 PM
I used to make beads on a hothead for a couple of years when I first started and mostly made encased ones, so it is possible. :)

Here are some made on a HotHead during my first year or so :

(http://kathryngreer.com/pix/auction4.jpg)

Your base bead has to be as cool as possible without it cracking when you encase and always remember not to put it in the flame while encasing (except a flash or two to keep it warm enough not the crack).
When I encase, the clear rod (I use any type, but mostly Effetre these days) is in the flame, while the bead is right under the flame, a little to the left so I can see what I am doing. I mostly use the wrap around method.
Title: Re: Encasing! ...or lack thereof
Post by: MadelineBunyan on February 16, 2011, 04:51:39 PM
I don't use a hothead, but I will say that the Mary lockwood tut is great, it explains lots of different ways of doing it, so you can find the one that suits you, or the bead.

I only really 'got it' with encasing relatively recently, I had to, cause I fell in love with encased silver glass!
I use reichenbach clear, and those tend to be fairly thin, 6mm or less.but as someone said they are quite stiff, but I find I get a better wrap around the bead when I can control it, too melty and its just a mess!(maybe cause I'm on a bobcat not a hothead, maybe on a hothead the amount of melty the 006 gets is just right...?)also, there were the problems with clear, until 006, and then reichenbach were available I never really encased anything except white with other colours, then decorated on top, like Kaz showed.

I encase spiralling around the bead, and unless its really long (ie its going to take me ages to get to the other end) I let it get pretty cool, (hold in dark place see if glow is gone) start at left, touch end of molten clear to bead, then I push the glass on (cause the reichenbach is firmer, also I get less bubbles) whilst turning the bead(which is underneath the flame), making sure it touches the previous wrap. for the pushing on method you need the base bead to be cold, or you're just gonna pull it all out of shape. I tend not to worry too much about how cold, cause I'm going to heat it all through after I'm done encasing (heat, then take out of flame to let heat go to the centre, then heat again, take out of flame again)
Title: Re: Encasing! ...or lack thereof
Post by: ScarletLeonard on February 16, 2011, 06:00:17 PM
Another vote for mary lockwood (if your lucky the 24 hour sale from earlier in the year is probably still going it was a little while ago)

I've found the best way for me on the HH (though you may find it doesn't work for you.) two coils from the rod around the centre of the base bead, then one coil from the rod on each side. I heat the sides and push it round with my pokey tool then take the whole assemble under the flame and only heat the clear.
For thinner encasing I use the same method but use a stringer.

The biggest trick is getting the base bead to stay put, practice with another trans colour over a base bead since other trans are softer then clear.

Patience is probably the key on a HH. It is slow but once you get the hang of it it doesn't seem as slow.
Title: Re: Encasing! ...or lack thereof
Post by: Redhotsal on February 16, 2011, 07:51:22 PM
Some simple encasing ideas:
1) Make the base bead really, really small.
2) Make the base bead a "lemon" shape as opposed to a "tyre" shape. That's much easier to encase as there are no undercuts.
3) Only encase the bits that need encasing - I used to be very bad at encasing on a hothead but wanted to make encased florals. I started with a base bead which was transparent (you can't see the join between a transparent bead and clear encasing) and then I put my florals on. Plunge the florals and then encase ONLY the florals. Much much easier and you end up with a reasonably sized bead, which of course, is much quicker to make.
4) Don't forget, encasing over an opaque with a transparent is always difficult because on the whole, transparents are stiffer and melt at a slightly higher temperature than opaques. This means your opaque is getting runny before the clear is and so will try and leech out round the sides of the encasing.
5) Yes, your base bead needs to be quite cool. If it's too hot the pattern of the base bead gets smeared.
6) If you have the patience try "dump encasing". Make the base bead and then hold it very high up in the flame. Take your cler rod and melt a huge gather - about the same size of the final bead size. Then you literally dump it over the base bead and smoosh it round with the rod until it covers everything.
Title: Re: Encasing! ...or lack thereof
Post by: AnnaSpanna on February 16, 2011, 08:23:50 PM
Early on in my HH learner stages I was really frustrated with my naff encasing skills. I decided to devote a week to encasing and vowed that every bead I made had to be encased until I got it. I decided to start with small base beads covered in frit. I chose frit because it meant if the encasing effort distorted the frit on the bead it would possibly enhance, as opposed to spoil, the design and appearance of the bead. I found this a really useful exercise and stuck to it religiously. By the end of the week I was able to evenly and thinly encase beads without totally distorting their design (although by this point I had progressed onto making small gravity patterned base beads - still using the frit to make the gravity bead) and subsequently these were the second set of beads I sold in my Etsy shop. It really is a case of PPP in this instance but as I said I did dedicate a week to it. I was really thankful that I did. i also found that it paid to get the glass super super hot at the end of the rod so that it would "squidge" further around the bead and be thinner. I also found that a 6mm red hot poker with a chisel end (Carl Martin tools - wibbly wobbly glass) is excellent for pushing and manipulating the clear around the bead to cover missed patches or just to even out the  thick and thin bits - I blogged about my encasing traumas - http://rainlilybeads.blogspot.com/2010/04/just-encase-youre-gettng-frustrated.html

There are many different methods of encasing and everyone has a favourite way, and one which simply doesn't work for them. Take on board all of the different methods and try them and see which one you prefer. Once you have got some more torch time under your belt you will find that you will begin to evolve your technique and be able to adapt it to the type of bead you are making. Do not fret and yes it can be frustrating. It is a hurdle that we have all gone through and once you have mastered it you will not look back. It really does just take PPP.

Good luck  ;D
Title: Re: Encasing! ...or lack thereof
Post by: Les on February 16, 2011, 08:27:32 PM
That's a great blog post .. thanks for sharing :)
Title: Re: Encasing! ...or lack thereof
Post by: DeanWilson on February 16, 2011, 10:22:06 PM
Thank you guys for all the help!! ;D I'm not being horribly ignorant (well I am :P)- I'm having a sleepover at a friends house which is why I haven't replied and thanked you all!! ;D these look like AMAZING methods and will hopefully remove my encasing woes when I'm back on the torch!! :P

Lovely example beads btw- really encouraging that you can do work that beautiful on a hot head :)

Dean ;D x
Title: Re: Encasing! ...or lack thereof
Post by: elburnzo on February 16, 2011, 11:44:08 PM
hmm a week of nothing but making encased beads.... i think i'll give tht a bash!
Title: Re: Encasing! ...or lack thereof
Post by: AnnaSpanna on February 17, 2011, 12:55:12 PM
I will admit that on about day 3 I nearly quit!
Title: Re: Encasing! ...or lack thereof
Post by: DeanWilson on February 20, 2011, 03:24:03 PM
Had a go with some of these methods and actually had a moderate degree of success!! :P Shocking!! :P ;D

Just had an idea though....Could you use clear glass frit to encase your beads? Very finely ground to give a really even coating? And because it's glass obviously it would all blend in evenly anyway! Has anyone tried this before?

Dean ;D x
Title: Re: Encasing! ...or lack thereof
Post by: MadelineBunyan on February 20, 2011, 04:11:11 PM
in glass casting, the bigger the chunks you use, the better clarity you get, and when you cast in frit, you get cloudy. I guess this would be the same with a bead.

you could try it, but you'll need to wash your frit very thoroughly, every speck of dust dirt grease, etc will probably result in scum,or some other unpleasantness. perhaps the results will be interesting, may take you down an interesting arty path, but sadly I dont think it will result in beautifully clear encasing.

encasing is a skill worth persevering with!