Hi, hope anybody can help me with this one.
I keep getting the same question from somebody who makes raised flower big hole beads and she wants to line these with silver cores.
As far as I know this is not possible when the sides of the beads are not in a nice pucker but maybe I'm wrong.
Are there ways to line a bead with a silver core if the surface is decorated with a raised design?
Thanks for helping me.
Nope ! you know as much as me Maria Louisa but the design needs to be away from the edge allowing for the silver if the puckers dont exist and the hole edges lean outwards then its much more difficult but Davids finishing dies do the trick ::) Trouble is we just havnt had time to produce them for sale >:(
Just need to make sure there is enough room round the hole to core without touching any bumps
(http://farm6.static.flickr.com/5058/5422030406_c4efd4ab52.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5422030406/)
IMG_0571 (http://www.flickr.com/photos/cheekycherubdesigns/5422030406/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Or use bead caps - this also works if the holes aren't perfect -although mine on tis one were :P so it's not a cover up job!
(http://farm6.static.flickr.com/5056/5421423833_b00388a9e4.jpg) (http://www.flickr.com/photos/cheekycherubdesigns/5421423833/)
IMG_0566 (http://www.flickr.com/photos/cheekycherubdesigns/5421423833/) by Kaz ~ CheekyCherubDesigns (http://www.flickr.com/people/cheekycherubdesigns/), on Flickr
Kazx
Those are lovely Kaz, especially the greenie.
Hi Manda,
I can't wait for the ones that David is making. Please tell him to hurry ;D.
Someone showed me something from the campingshop last week which she used to core faceted precious stones which worked. So I'm planning to do a little campingshoptrip next week.
Kaz, gorgeous beads.
That's the way I told her now to make her beads.
Surface at the top, not at the sides.
You wouldn't want the decoration on the sides round the hole anyway, even if it were not cored it would bump into the beads on either side which would increase the chances of the raised bits breaking.
I've always wondered about the caps, as they cover the nice dimples, but lots of people do cap then core.