Title: Silver Core rivets!
Post by: DeanWilson on February 06, 2011, 02:09:49 PM
Hiya guys, I know there's a thread already about silver cores with piping etc but I was wondering about rivets that you can just buy- eg these on Tuffnells: http://www.tuffnellglass.com/contents/en-uk/d28_tuffnellglass.com_01.html (they're at the bottom of the page)

I was just wondering how on earth they're used! Do they just pop in or do you need glue or something and then is it some special glue?  ??? A bit confuzzled as I'd love to make some Pandora style beads for my big sister and would really like them to look the part  ;) ;D

I've actually ordered some (the cheaper 'style' rivets, silver plate I think) that should arrive on Tuesday I think so I'm jumping the gun a bit here and might work it out myself- but it's probably better I ask some of you amazing professionals before I learn myself, going through 10 pairs in the process :P

Thanks a lot in advance :D Dean ;) xo
Title: Re: Silver Core rivets!
Post by: poledra1958 on February 06, 2011, 02:14:14 PM
You glue them in as far as I know.  Have only used them with polymer clay so far.   ;D 

One day I may be able to make a big hole bead that I think is good enough to core.

Jenny
Title: Re: Silver Core rivets!
Post by: jobead on February 06, 2011, 02:17:05 PM
Hi Dean
Yes you just glue them in, you are probably best using two part epoxy which you can get off jewellery making or craft websites. I've used other super glue type stuff but it doesn't seem to work as well.

The rivits are the easy bit, it's the big hole beads that are tricky  ;)
Title: Re: Silver Core rivets!
Post by: DeanWilson on February 06, 2011, 02:19:02 PM
Oh well that's fine, thanks a lot  ;D I was worrying about some press and piping and flaring and what?! :P All over my head as I don't even have a kiln yet so glue is just fine for me  ;D

Thanks a lot ladies!!  ;) ;D
Title: Re: Silver Core rivets!
Post by: julieHB on February 06, 2011, 02:21:56 PM
The araldite crystal clear is a cheap and easily available two-part epoxy that does the job well.  :)
Title: Re: Silver Core rivets!
Post by: SilverGems89 on February 06, 2011, 02:41:43 PM
I use araldite clear 2-part epoxy that i got from B&Q, really simple to use, although you have to be quick because it goes off really quickly (will look for slower curing stuff next time) but i havent had any problems with it
Title: Re: Silver Core rivets!
Post by: DeanWilson on February 06, 2011, 02:55:10 PM
Brilliant thanks, will look out for it! :D
Title: Re: Silver Core rivets!
Post by: GaysieMay on February 06, 2011, 03:41:41 PM
You can also use a glass glue that comes in one part, I get mine from Wilkinsons, its like a small tube of super glue just called glass glue but you need a sunny day for it to go off, something to do with ultra violet light.
Title: Re: Silver Core rivets!
Post by: Blue Box Studio on February 11, 2011, 05:10:52 PM
Don't bother with the Scotch £20+ a pack stuff from some places though, I find it doesn't stick nearly as well as Araldite, goes gloopy in the dish far too quickly and gets everywhere.

Is there an antedote to epoxy glues?  What's 'rubbing alcohol'?