Hello- I hope this is in the right place! I was just wondering if anyone would have any pointers for me on off mandrel sculpture? I can make beads okay but anything without a mandrel totally daunts me! I had a friend who used to make little frogs on marbles etc but they're too difficult! :( Maybe because I don't have a marble mould yet but I can't even seem to do a lentil bead (just with a knife and a graphite block to flatten) properly! I know it's a long shot but any help would be appreciated :D
Dean x
Hi Dean
Now first up I should say that I've never attempted off mandrel in my life, so I'm no expert ;D However, my understanding is that you actually have the glass attached to the mandrel until the end, and then you melt that last little bit off in the flame and shape if you see what I mean.... so you'd make your round bead right on the end of your mandrel, then your frog on that then melt off the last bit of glass right at the end....
I think, anyway. ??? Someone more knowledgeable will be along shortly! ;D ;D ;D ;D ;D
Oh wow! That's brilliant that there's more than one way to do it! ;D My friend made a huge gather on a rod itself, shaped it in a marble mould, did the frog or whatever, attached a punty to the other side, reshaped, polished etc and attached a loop to hang as a necklace ;D I've tried but as of yet I'm rubbish! ;D It's great being here talking to people who have first hand experience who know what I mean :D this forum is fab ;D ;) Thanks a lot :) x
Hey Dean,
Personally I found one of the easiest off mandrel things to do when I first started was a heart pendant.
As you say it is formed on the end of a rod and then once you have completed your shaping you cut it off in the flame creating the bottom of the heart.
I shall see if I can find the tutorial on Lampwork etc for you.
Here you are:
http://www.lampworketc.com/forums/showthread.php?t=591&highlight=mandrel+heart (http://www.lampworketc.com/forums/showthread.php?t=591&highlight=mandrel+heart)
Thanks a lot Stacy will check it out!! ;D x
Can't really add much more than what Helen has already said. You can always use a glass rod as a mandrel and form your object on there, then flame cut it off. If you use soft glass you'll have to try and keep it all warm so it doesn't shock and break.
Leaves are really easy and fun off mandrel object to make, melt a nice blob on the end of a rod, flatten into a lollipop with mashers. You'll need to re-heat it to get rid of any chill marks, although somepeople like them so leave them. I then use a pair of old scissors to 'cut' veins (don't go too hard as you are just creating dents in the glass, you don't want to cut through them.) Then I make a longer 'cut' for the centre vein and then using tweezers, scissors, or another rod pull the leaf to a point. It's then just a matter of flame cutting the leaf off the rod (flick it over for a loop, takes some practise but well worth learning) and pop it in the kiln.
Hope that makes sense, there is a link here with some photos (which probably makes more sense than my ramblings! ;D) http://www.marylockwood.com/files/offhandleafprintquality.pdf (http://www.marylockwood.com/files/offhandleafprintquality.pdf)
That sounds really great thanks, will definitely give it a go! ;D x
Off mandrel stuff is fun ;D ;D I would personally find it easier to do the whole lot on a glass rod but I was taught that way and it just comes naturally now. It takes practice to get the hang of the heat flow and I agree with Stacy, an easy thing to start with is a heart. The arrowhead or heart tutorial by Shari Slonski is great for starting to 'get' heat flow while still having the comfort of a mandrel.
Otherwise, there are a bunch of off-mandrel demos on Youtube and there was a guy who did several really nice off-mandrel animal tutes which might get you started...http://www.marshglass.com/ (http://www.marshglass.com/) though I'd maybe try one of the easier ones first, like the dolphin ;)
There must be off-mandrel goddess tutes somewhere too.....
Yup, I've been making hearts from Mr Smiley's tutorial and they're very addictive! (There are photos further on in the link Stacy gave). The loops are the hardest part!
I've also been doing some implosions - Scott Young has a tutorial on WetCanvas (http://www.wetcanvas.com/forums/showthread.php?t=170943). I do have a doming block that I've been using to shape them, but I'm trying to make half-round pendants with flat backs.
It's fun but scary ;D
Dean, start small. Take a rod, heat a blob of glass and smoosh it down so you have a disk, that disk can be the start of lots of things. If you heat it right through and attach a rod to the tip and pull then you have made a leaf. If you add four small blobs and a big blob then you have a turtle. If you heat it and cut it using ordinary kitchen scissors then you have a flower.
The whole rod with the work on the end can go into the kiln until you need it again.
When I make loops I keep a brass rod to hand, I pull out the strand of glass, let it firm up slightly then pull it back down to meet where it comes out of the finished piece, burn it off and then SLOWLY go back into the flame, heat the loop just a little and push the rod through for evenness.
If you get panicky about making loops, make a bead on a mandrel and put it in the kiln, then make your off mandrel piece, take the mandrel with the bead on it out of the kiln and heat the two areas where the bead and the piece will meet, join together and you have a neat loop!
Thanks for all your advice! You're definitely right to start small I think, I always try to do things that are far too difficult and end up with my fingers burnt! My goal I think is to make off-mandrel goddesses; I've seen a few and they are just stunning! I still struggle with on mandrel ones and, as I'm on a hot head the amount of time it takes to melt the sheer amount of glass required annoys me >:(
Thanks for the tut Tan and the links guys :)
Dean ;D
Actually, with something like a goddess you work from one end to the other, you wouldn't need to melt all the glass at once - which would help on a HH! The thing with bigger/more complex soft glass sculptures is to work from one end of the piece to the other so that once you have finished a part, you let it cool and don't reheat it (reheating will cause thermal cracking). I am probably not explaining it well, will have a look later and see if I can find a tute.
Made some off mandrel pieces...Mostly just experimenting, tried to make a yellow and white daisy...It went HORRENDOUSLY wrong and now I have an equally horrendous woman's face thing I made with yellow-white skin and blue hair XD It's awful :P Will check if they're cool enough from the fibre blanket and snap a few pics ;D
Making crap is how you learn ;)
Absolutely :) Experimentation breeds genius and there's nothing wrong with a few bits of crap on the way :)
Righteyo, putting a load up here...Quite proud of the goddess, have never attempted an off-mandrel one before! The violet drop I know is destined to break but I thought it was pretty :P I quite like the duck-thing I made too ;D It has a wee crown :P Anyway you guys can see for yourself :) I made an awful in your face leaf too XD And the weird face :D :D You can DEFINITELY tell I made it first :P
AAAH!!
(http://farm6.static.flickr.com/5214/5422918164_867d6ca1bf.jpg) (http://www.flickr.com/photos/deans_photography/5422918164/)
DSC00283 (http://www.flickr.com/photos/deans_photography/5422918164/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
Not much better :P
(http://farm6.static.flickr.com/5052/5422924022_f73d755f9b.jpg) (http://www.flickr.com/photos/deans_photography/5422924022/)
DSC00272 (http://www.flickr.com/photos/deans_photography/5422924022/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5054/5422321171_c29d306573.jpg) (http://www.flickr.com/photos/deans_photography/5422321171/)
DSC00282 (http://www.flickr.com/photos/deans_photography/5422321171/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5293/5422320389_eabdb9e328.jpg) (http://www.flickr.com/photos/deans_photography/5422320389/)
DSC00279 (http://www.flickr.com/photos/deans_photography/5422320389/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5018/5422926242_b8ec1618a6.jpg) (http://www.flickr.com/photos/deans_photography/5422926242/)
DSC00277 (http://www.flickr.com/photos/deans_photography/5422926242/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5171/5422925384_19bf91d7de.jpg) (http://www.flickr.com/photos/deans_photography/5422925384/)
DSC00275 (http://www.flickr.com/photos/deans_photography/5422925384/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5139/5422920110_9bc4379145.jpg) (http://www.flickr.com/photos/deans_photography/5422920110/)
DSC00259 (http://www.flickr.com/photos/deans_photography/5422920110/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5254/5422919584_e701850005.jpg) (http://www.flickr.com/photos/deans_photography/5422919584/)
DSC00258 (http://www.flickr.com/photos/deans_photography/5422919584/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5252/5422312851_888fe722bb.jpg) (http://www.flickr.com/photos/deans_photography/5422312851/)
DSC00257 (http://www.flickr.com/photos/deans_photography/5422312851/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
Quite hard to photograph properly this one...Quite happy with it :P
(http://farm6.static.flickr.com/5134/5422923332_0eff219211.jpg) (http://www.flickr.com/photos/deans_photography/5422923332/)
DSC00269 (http://www.flickr.com/photos/deans_photography/5422923332/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5297/5422921788_64bf602325.jpg) (http://www.flickr.com/photos/deans_photography/5422921788/)
DSC00265 (http://www.flickr.com/photos/deans_photography/5422921788/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
(http://farm6.static.flickr.com/5180/5422314785_2b8496cb29.jpg) (http://www.flickr.com/photos/deans_photography/5422314785/)
DSC00264 (http://www.flickr.com/photos/deans_photography/5422314785/) by DeanWilson (http://www.flickr.com/people/deans_photography/), on Flickr
Pfft! Lots of photos!! :P
I like the duck a lot, it has character! :D
That goddess ain't half bad either :)
Haha wow thanks so much!! :O :o ;D ;D That's a huge compliment :P And I'm sure I'll get better after a while :D Well, I hope at least ;) :P
I like the duck too. ;D
Check out Wesley flemming with his bug's. I would like to be at his level of glass control and skill sometime.
I admit when you said on another thread that you made goddess beads I did wonder what a teenage boys take on a goddess bead would look like ;D And I must say I love your goddess pendant and your duck has a great personality.
If you have not seen it already check out http://www.frit-happens.co.uk/forum/index.php?topic=2261.0 it shows how peoples work has progressed.
Thanks a lot ;D Just looked at his webpage, wow!! :O Gross and they creep me out but amazing skill involved! I'd have to have been lampworking in the womb to get to his standard :P
Hiya Dean, you've been amazingly busy and your beads look pretty good, possibly a silly question but... (I'd rather ask than sit here puzzling my brain cell all night) what do you use to get your off mandrel glass creation into the kiln, assuming at that point your punty rod has been removed?
see I told you it was a daft question, sorry!
kath
Good work Dean
Thanks Tan and Kath! ;D
Oh god way to single me out as an amateur Kath :P I don't have a kiln! :O ...Yet ;) :D I'm just using fibre glass blanket as of yet (although my Japanese cooling bubbles arrived TODAY!! ;D) and I just picked 'em up with forceps and popped it in :P Although you could so the same with a kiln :P The forceps were given to me by a friend and I find them invaluable, in fact I thought everyone used them! (do you? :P) I guess you could use tweezers too if you had a hole in it too :)
I use whatever is laying nearest my panicking hand :D
I've been making stuff with loops so I use my pliers to hold the loop.
Do you warm them first? I do but sometimes it doesn't seem to make much of a difference? I have some very nice long tweezers that are a bit finer and seem to be alittle kinder on the glass.
Hmm, when I remember! They're needlenose pliers and not usually freezing cold to start with because I use them for all sorts. Haven't had them shock anything yet, anyway.
ETA: Actually, by the time I hold loops with them they're definitely warmed, because I use them to try and keep the inside of the loop round after I've put it on! Don't have any graphite rods yet.
I think my tools are just shocking...........its the abuse I give em :D
Actually, I wondered about using a wooden peg to hold things? They are nice and pinchy and shouldn't shock anything, wondering if they would need to be waterlogged first?
I'm also working indoors in a nice heated kitchen, so... ;D
I was just curious as I'm still in the it's got to be on a mandrel stage!
thanks for the answers. :)
kath
Basically, the glass rod becomes the mandrel and you work off the tip rather than around it....if that makes sense?
kind of!
I think I'll have to find a video or watch someone to really get it sorted in my head :D, thanks Tan, I'm off to you tube now!
kath
Am I right in thinking that working on a rod (no mandrel in sight) the glass is less prone to shocking.
What I mean is, because there is no metal mandrel heating up and down inside the glass.... just a lump of glass.... heat/glass is more stable?
Might of read that from somewhere.
Denise
From my, oooh, whole week of doing this, it does seem to feel that way :D
I've had a couple of things I was expecting to hear little cracking noises from that were absolutely fine when I put them back in the flame. It also makes me work rounder, so the glass is thicker and the core retains heat longer. Certainly compared to a pressed bead.
I would think wooden pegs might need to be waterlogged.
You do still have to be careful to avoid thermal shock off-mandrel, but the thicker core of glass does seem to hold the heat. I'd never really thought about the metal making the glass less stable but it would make sense.
I have the marvellous ability to shock both on and off mandrel (boro that is) ;D
I hate that tink
Yes, and it always happens after you've been working on something for over 40 minutes >:(
And then................you go back and think.......I can just fix that crack and as you hit it with heat either side cracks, then either side of that and either side of that
Loking at things from another angle I have never worked "on mandrel" but I suppose for those that use mandrels I must work off it. I have never thought about it that way. Its hard to "unlearn" sometimes but for those that want to, just stick any glass in flame, heat, twist and shape, blow, strectch do whatever. Imagine a 3D canvas with no size limits and fill it as much as possible.
Ian
Ian, the idea of going as big as you want really appeal's to me, but I love working small. I wish there were more soft glass sculptural teacher's in the uk to show me some trick's.
I look at sculpture's done by Wesley Flemming and think, how does he do that and not have to keep flashing the entire glass piece in the flame to keep it warm? In his video he hold's the bug he is working on with his hand's... I would love to work like that. Making one bit, then making another bit the next day.
Denise
I think the Glass Artistry DVD from Bob Martin shows him using wooden pegs to hold his animals. I don't think, from the looks of them that they were water soaked. Large items that won't fit through the bead door, I just open the main door very quickly and pop the item in.
Who is Bob Martin Pat?
Bob makes a lot of glass animals in soft and I have seen him make dragons, horses, etc.. from Borosilicate. Used to work for Pirelli or however the tyre company is called. Been making glass for years. teached at Plowdens and has great DVD out. Demoed at BSSG Symposiums. Photos of his work in GBUK Journal.
I have worked on sperate pieces and then joined them all up in flame. trick is flame control. Just made a parachutist and trick there was only heat the part of glass that you want to seal togtaher. can hold with fingers if wholoe is not hot. Largets items I have made are about 24 inches long plus
Sorry for spelling but in a ruch
Ian
Thanks Ian, I shall give him a google ;)
Quote from: Tan on February 10, 2011, 01:37:45 PM
Who is Bob Martin Pat?
Doesn't he make worming tablets for dogs? ;D ;D ;D
I have to admit thats what I thought :D
Any ideas as to where you can get that DVD???
A google shows Sal stocks it
http://www.lampworkbeads.co.uk/page6.htm
Thanks for the link ;D
Bob's contact info on the back cover of the DVD case is www.chixglass@tiscali.co.uk and you can see his horses at http://www.acclaimimages.com/_gallery/_pages/0028-0602-0606-1405.html