I watched Kaz's tutorial this morning on applying murrini. Which I thought was fab :) Off I go to The Arctic to give it a go :)
The first 2 went on fantastically...the 3rd however stuck to the tweezers creating a lovely swirly pattern, which if it had been what I had intended would have been lovely!! Anyway I tried again and again and again all with sticking to tweezer results.
What am I doing wrong please? :)
sarah x
Hi Sarah
It may be that the tweezers are getting hot and therefore the glass is sticking. Perhaps dunk them in your water jar from time to time. Alternatively, once you have place the murrini onto the bead with your tweezers, then gently use your graphite marver or other flat graphite tool to press them on (very gently). You need to be careful with this as the marver is a big tool to do a small job and the amount of pressure you exert needs to be proportionate to the teeny murrini chip! I have a little tool that Diane T's husband made me which I call a murrini (or dot) dobber. It is a wide thick ended brass screw which has been levelled off to take out the screw groove and then screwed into a little wooden handle. It is perfect for the job!
Keep going - they do take a while to get used to using, but once you have you can get amazingly clear results (I have to say that I think Julie HB's application of murrini far surpasses mine as I still occasionally get a bit of blurring through rushing!)
Kazx
Thank you :) The tweezers were getting quite hot, so will give it ago again :)
XX
1) you may have heated the tweezers so much when you prewarm your murrini that it sticks - just waft it in and out of the flame a bit before applying, that should be enough. To make sure you avoid the tweezers being too hot before you pick up a new murrini you can dunk it in water after application of each murrini. I have never found this necessary, though.
2) Remember to apply the murrini to the bead outside the flame! The chances are that you will ruin your tweezers pretty quickly otherwise (as well as making a right mess of applying the murrini, of course)
HTH :)
It does take some practice - I apply mine with self locking tweezers, gently heat and I use my marver to press (when I say press it really is very gentle, more of a rest on the marver) – I leave it on for a count of two and I repeat this several times till I'm happy with the application.
I used to get my murrini quite blurred, but holding it for the count of 2 each time gives the glass a chance to "set up" properly.
Yep that happens to me too, the murrinis too hot and the tweezers probably too. All sorts of things happen with my murrini ::) but I love them so and am persevering and I get it right sometimes too. :)
A dunk inbetween uses for the tweezers and I have a little crow bar tool from Mandas which is perfect for patting as has 2 ends different sizes and is graphite.
I have some other murrini, ie not Kazs and find it gets hot very fast and blurs right away, I dont know if they are different types of glass or what but they seem more fragile and shock and break easier. Kazs seem to take quite a bit of manhandling usually. :)
But I do try to be gentle.
Thank you all so much. I knew that in the time it took to empty the washing machine and make a cup of tea I would have been rescued.
MWAH :) xx
I use one of Manda's tools for patting down murrini (and for encasing, tidying bead ends, general prodding where you want something smaller than a marver). Bead shaper (http://www.mangobeads.co.uk/index.php?page=shop.product_details&flypage=flypage.tpl&product_id=5&category_id=27&option=com_virtuemart&Itemid=2&vmcchk=1&Itemid=2). There's also one with a lake (pointy end) at the other end.
Thanks, Kaz!! :-*
I do mostly use my marver when flattening the murrini, and sometimes a knife. As Kaz says, it is VERY easy to blur the murrini when applying. It is a skill of patience and love! :D In particularly the first few taps I go ever so gently, and I work cool.
This has been helpful for me too , thanks. :)
Yea it worked, cold tweezers and some water...such a difference Thank you :)
You're welcome ;) Photos when they're cooked please!