Bluestone and Goldstone does it have to be encased or can you heat it from the flame. I did some but encased just incase it burnt ???
You can leave it unencased, heat it enough to be sure it's firmly attached.
It just can't take long periods in the flame. I used to think that goldstone couldn't go in the flame and was a bit afraid of it. But it can take some heat, but too much time in the flame will burn out it's sparkle!
Morning Trudi , Long time no here. How are u .
Thanks for that I shall have a go today. It was either cleaning , hubbys paperwork so I thought I would go play with glass instead !!
Off to get dressed
Enjoy!
Is still not brave enough to try goldstone...
have fun at the torch and good luck with your playing (photos please) I would love to be with mine now but still got wee man running around.
I had some goldstone on last weeks gallery with mermaid encased . second to last page i think.
I have had a short go without encasing so shall post on gallery if good tom . Fingers crossed ;D