I want to make a bead that is a rich purple. None of the purple shades i have are rich enough.
Is there a glass I can buy, or will I have to layer the colours to get a royal transparent purple look?
Please help if you can....thanks
Effetre dark trans violet over White is good but if you want an opaque try Reichenbach opaque lilac - it sounds too pale, being called lilac, but it's not. It's my new fave purple!
I've tried CIM (I think) blackcurrent over white and that gives a good deep purple. :)
effetre dark violet is nice but can be a bit navy blue-ish.
light violet is a better purple, but obviously lighter.
(http://madelinebunyan.files.wordpress.com/2010/10/dscf1687bobblesandfinssm.jpg?w=300&h=197)
the little purple heart bead here is light violet, over white or possibly baby blue. but if you encased thicker you should get a nice rich colour.
Cim Grape Ape is quite a nice purple, but it might not be rich enough for you. If I want really deep rich purple I layer amethyst over effetre periwinkle (tip from Corina :))
I also love ink blue - tis actually purple
(http://farm5.static.flickr.com/4103/4957718906_43e87faa97.jpg) (http://www.flickr.com/photos/glitteringprize/4957718906/)
Chocolate Box Love (http://www.flickr.com/photos/glitteringprize/4957718906/) by Glittering Prize - Trudi (http://www.flickr.com/people/glitteringprize/), on Flickr
looks like velvet when you etch it!
(http://farm5.static.flickr.com/4008/5078188905_9f4f6ea57e.jpg) (http://www.flickr.com/photos/glitteringprize/5078188905/)
Blueberry Marble Rounds Light (http://www.flickr.com/photos/glitteringprize/5078188905/) by Glittering Prize - Trudi (http://www.flickr.com/people/glitteringprize/), on Flickr
Trans Dark violet is lovely for a transparent purple
Not entirely helpful but for opaque CiM Eggplant it's a beautiful rich colour and my favourite purple it's also got a luscious shine to it. I've used it dotted on clear and it keeps it's deep colour but goes translucent so it may be one to try as a thin encasement over clear.
CiM Blackcurrant is a little dark for my tastes it ends up nearly black on it's own. I've not tried that over white though (guess what I am doing later)
I completely agree CIM Blackcurrent is basically black unless you put it on top of something else.
Ooooh, Trudi, I love that heart!!! And you have just reminded me, I love ink blue as well!! ;D ;D
Quote from: Lush! on January 18, 2011, 09:29:46 AM
Effetre dark trans violet over White is good but if you want an opaque try Reichenbach opaque lilac - it sounds too pale, being called lilac, but it's not. It's my new fave purple!
I've been trying to get hold of some - where do you get yours?
Quote from: julieHB on January 18, 2011, 01:29:09 PM
Ooooh, Trudi, I love that heart!!! And you have just reminded me, I love ink blue as well!! ;D ;D
I think that the camera lense reflection really sets it off :) Ink blue is a gorgeous colour, reminds me of cadbury's!!
Mandy - I think Martin stocks it, look under specials/handpulled!
Quote from: Mand on January 18, 2011, 02:02:44 PM
Quote from: Lush! on January 18, 2011, 09:29:46 AM
Effetre dark trans violet over White is good but if you want an opaque try Reichenbach opaque lilac - it sounds too pale, being called lilac, but it's not. It's my new fave purple!
I've been trying to get hold of some - where do you get yours?
If you mean the Reichenbach, Mand, Tuffnells have it - or they did last week!
Oh the heart is lovely. The colour is just what I am looking for!
I have some black currant, and I tried it this afternoon over white, i also tried it with a bit of Transparent amethyst over the top. ( I think I need it to be a bit more of a bluey purple, and this looked more of a red/purple)
I will have to see what its like when it comes out of the kiln, but it looks promising.
Tomorrow i will try amethyst over periwinkle.
Thank you for all the suggestions, but some I cant try as I havent got the right colours. (yet) :D
I have just bought some Effetre Ink blue and also some Blue Purple which looks darker. I am more than happy to send you a rod of each Shirl, if you would like try them out.
Quote from: cbeadies on January 18, 2011, 04:32:00 PM
I have just bought some Effetre Ink blue and also some Blue Purple which looks darker. I am more than happy to send you a rod of each Shirl, if you would like try them out.
Thats so sweet of you thank you. Is there anything that you would like me to send you in return?
PM ing you! :)
ink blue definately reminds me of the colour of cadburys too! its one of the very very few transparent colours that i like ;D
Quote from: Lush! on January 18, 2011, 02:36:40 PM
If you mean the Reichenbach, Mand, Tuffnells have it - or they did last week!
I tried ordering some but it was out of stock :( On the plus side my Flame Off ticket arrived though! ;)
Ah, oops, sorry :-[
Trudi that purple heart is gorgeous as are the etched beads. I've been looking for a good purple too so this is a great thread.
The blackcurrant over white is quite good, but not quite the cadburys chocolate colour I am after. I am going to have another play now.
Cheadies has very kindly offered to send me something she thinks will be the right colour. many thanks :-*
I am trying to make a bead for someone as a surprise gift, and want it to be right for her.