Frit-Happens !

Lampwork => Common Problems => Topic started by: Lotti on January 06, 2011, 10:11:41 AM

Title: Getting bead release out of hollow beads
Post by: Lotti on January 06, 2011, 10:11:41 AM
So been having a play and managed to make a (rather large) hollow bead yesterday (the puckers need a bit of work, but am so pleased that I managed to make it and it didn't collapse), got it off the mandrel fine this morning, but there is a big lump of bead release stuck in the middle.  Currently I have the bead soaking in water in the hope that the bead release inside the bead (there is water inside the bead) will eventually liquidise and I can poor it out.  How do other folks get bead release out of hollow beads?  Thanks, Lotti :)
Title: Re: Getting bead release out of hollow beads
Post by: MangoBeads on January 06, 2011, 10:18:57 AM
Thats the best way Lottie just keep rinsing through to dissolve it and eventually you will get rid - well done you ! Keep shaking it to dissolve it ...
Title: Re: Getting bead release out of hollow beads
Post by: Lotti on January 06, 2011, 10:29:55 AM
Thanks Manda.  Been having quite a play indeed!  Will be needing some help with encasing, just can't get the ends covered.  Will post my week's attempts on the gallery at the weekend!  Kiln back on, might try to make some smaller hollow ones (got a bit carried away) and maybe a set!  Will see how I get on, but jolly chilly out there again. :)
Title: Re: Getting bead release out of hollow beads
Post by: MadelineBunyan on January 06, 2011, 10:38:13 AM
ok, heres what I do....

put bead under water and let it fill up.

put your thumb over the top hole. lift up over water bowl/sink

get a skinny mandrel, smaller than the one you made it on, and use it to break the surface tension in the bottom hole, also at this point you can let go of the top hole.

this makes the water come out fast and bring loose debris with it.

also, if you can get said small skinny mandrel in and poke the bead release lumps so the break up it will make it easier.

rinse and repeat!

also soaking out the water with rolled up bits of kitchen roll helps.
Title: Re: Getting bead release out of hollow beads
Post by: Trudi on January 06, 2011, 11:34:56 AM
I have some small pots (old yogurt ones) I fill the water just to cover the bead and I swirl it! The swirling tends to force out the bead release quite easily. If some bits are too big I give them a little poke with a mandrel to break them up and swirl again!
Title: Re: Getting bead release out of hollow beads
Post by: Redhotsal on January 06, 2011, 11:41:15 AM
This works a treat but can be messy if you slip. My husband holds the bead right over the outlet on the tap and turns the water on quite high. The resulting water pressure forces the debris out in no time. You just have to be careful not to let the bead slip or you'll be cleaning water off the windows/wall/yourself.
Title: Re: Getting bead release out of hollow beads
Post by: Amber on January 10, 2011, 04:27:00 PM
Canned air is pretty good  :) Best do this outside though, you don't want to inhale the bead release!