Frit-Happens !

Lampwork => COE 104 => Topic started by: Les on January 06, 2011, 09:01:21 AM

Title: Could someone just remind me ...
Post by: Les on January 06, 2011, 09:01:21 AM
Is it Laushca that doesn't get on with some glasses when used as encasing ?
Title: Re: Could someone just remind me ...
Post by: sparrow on January 06, 2011, 09:04:05 AM
yup :)
Title: Re: Could someone just remind me ...
Post by: Les on January 06, 2011, 09:05:20 AM
Arse ! .... must have got the rod mixed up by mistake then ... at least I know it's not me .... damn nice beads they were too
Title: Re: Could someone just remind me ...
Post by: Shirley on January 06, 2011, 05:13:20 PM
I use Lauscha transparent successfully when encasing effetre and some CIM. I've used it a fair bit with psyche and ekho as well with no problems. What were you making, Les?
Title: Re: Could someone just remind me ...
Post by: Les on January 06, 2011, 05:44:47 PM
just some florals over encased frit
Title: Re: Could someone just remind me ...
Post by: Shirley on January 06, 2011, 05:54:20 PM
you should be fine as long as you haven't been heavy-handed with the frit. I always use Lauscha to encase by floral beads, so if they haven't cracked they probably won't, unless you used a strange combo.

Think you need to show us!
Title: Re: Could someone just remind me ...
Post by: Les on January 06, 2011, 06:14:48 PM
I'll get a photo tomorrow