Frit-Happens !

Lampwork => Common Problems => Topic started by: The Tartan Trout on January 02, 2011, 12:13:26 PM

Title: ***WARNING*** tiny brain alert!!
Post by: The Tartan Trout on January 02, 2011, 12:13:26 PM
OK so everything that Santa brought is finally set up...unfortunately I wasn't good enough to receive a new brain or any common sense this year...please excuse me on this.

So the burning question for today in my tiny mind is....how long do beads have to be in the cooling bubbles before I can take them out for annealing ( or binning) I am in the garage in 'peanut smuggeling' temps if this makes a difference.

Thank you in advance lovely people with brains

Sarah xx
Title: Re: ***WARNING*** tiny brain alert!!
Post by: Les on January 02, 2011, 12:22:19 PM
It depends on the size of them :) I've never used the bubbles myself, but I used to leave it for a good 2 hours in vermiculite before checking :)

HTH ?
:)
Title: Re: ***WARNING*** tiny brain alert!!
Post by: Rainbow1 on January 02, 2011, 01:03:14 PM
I do most of my bead making in the evening, so I tend to leave the beads in the annealing bubble overnight. I work in our garage and bring the container with the annealing bubble into the kitchen when Iv'e finished. That way I can look at then in the morning.

Jo x
Title: Re: ***WARNING*** tiny brain alert!!
Post by: Fruddy on January 02, 2011, 01:54:39 PM
I used Annealing Bubbles for a couple of months when I first began and was kiln-less....

Just to be on the safe side, I would say wait a minimum of about 4 hours before having alook at them,hard as it may be to do so.  I lost quite a few beads when I first started, because I couldn't resist pulling the mandrels out for a second or two to have a look.

Here's a tip as well, - if you can, get yourself a genuine terracotta plant pot - they keep the heat in for much longer and let your beads cool much more slowly.
Title: Re: ***WARNING*** tiny brain alert!!
Post by: The Tartan Trout on January 02, 2011, 02:05:37 PM
Thank you :) I do have a kiln...the prometheus 7 but went to switch it on for the first time today and it doesnt work :( Have checked fuses but nothing...need to wait till Tuffnells open in a couple of days.
Title: Re: ***WARNING*** tiny brain alert!!
Post by: Fruddy on January 02, 2011, 02:08:16 PM
Quote from: The Tartan Trout on January 02, 2011, 02:05:37 PM
Thank you :) I do have a kiln...the prometheus 7 but went to switch it on for the first time today and it doesnt work :( Have checked fuses but nothing...need to wait till Tuffnells open in a couple of days.

I've got a Prometheus Pro-7 as well - when you say it doesn't work, is it totally dead when you go to switch it on?
Title: Re: ***WARNING*** tiny brain alert!!
Post by: sarah t on January 02, 2011, 02:10:46 PM
i thought you had a kiln so could not understand why you were using bubbles than annealing .....

fruddy has a pro 7 pm her see if she has any ideas...it would be really bad luck for it not to work ...might be something simple you have not done

cross posted but posted anyway  ;D

Title: Re: ***WARNING*** tiny brain alert!!
Post by: The Tartan Trout on January 02, 2011, 02:12:32 PM
Quote from: Fruddy on January 02, 2011, 02:08:16 PM
Quote from: The Tartan Trout on January 02, 2011, 02:05:37 PM
Thank you :) I do have a kiln...the prometheus 7 but went to switch it on for the first time today and it doesnt work :( Have checked fuses but nothing...need to wait till Tuffnells open in a couple of days.

I've got a Prometheus Pro-7 as well - when you say it doesn't work, is it totally dead when you go to switch it on?

yes competely dead...no noise no lights no heat no nothing :( i could be being thick...it wouldnt be the first time :)
Title: Re: ***WARNING*** tiny brain alert!!
Post by: Fruddy on January 02, 2011, 02:20:45 PM
Quote from: The Tartan Trout on January 02, 2011, 02:12:32 PM
Quote from: Fruddy on January 02, 2011, 02:08:16 PM
Quote from: The Tartan Trout on January 02, 2011, 02:05:37 PM
Thank you :) I do have a kiln...the prometheus 7 but went to switch it on for the first time today and it doesnt work :( Have checked fuses but nothing...need to wait till Tuffnells open in a couple of days.

I've got a Prometheus Pro-7 as well - when you say it doesn't work, is it totally dead when you go to switch it on?

yes competely dead...no noise no lights no heat no nothing :( i could be being thick...it wouldnt be the first time :)

No, you're not being thick at all.

When you switch the kiln on, the digital display should flash three times and then come up with the existing kiln temp.  They don't make any noise at all and don't produce any heat until you programme it, but the digital display should certainly come up straight away.

It could well just be something as simple as a loose wire, but as you have checked the fuses and no joy, then you are doing the right thing in waiting to contact Martin.  Hope you get it sorted soon.
Title: Re: ***WARNING*** tiny brain alert!!
Post by: The Tartan Trout on January 02, 2011, 02:26:21 PM
Quote from: Fruddy on January 02, 2011, 02:20:45 PM
Quote from: The Tartan Trout on January 02, 2011, 02:12:32 PM
Quote from: Fruddy on January 02, 2011, 02:08:16 PM
Quote from: The Tartan Trout on January 02, 2011, 02:05:37 PM
Thank you :) I do have a kiln...the prometheus 7 but went to switch it on for the first time today and it doesnt work :( Have checked fuses but nothing...need to wait till Tuffnells open in a couple of days.

I've got a Prometheus Pro-7 as well - when you say it doesn't work, is it totally dead when you go to switch it on?

yes competely dead...no noise no lights no heat no nothing :( i could be being thick...it wouldnt be the first time :)

No, you're not being thick at all.

When you switch the kiln on, the digital display should flash three times and then come up with the existing kiln temp.  They don't make any noise at all and don't produce any heat until you programme it, but the digital display should certainly come up straight away.

It could well just be something as simple as a loose wire, but as you have checked the fuses and no joy, then you are doing the right thing in waiting to contact Martin.  Hope you get it sorted soon.

Oh Good :) sometimes i do wonder what happened to my once quite clever brain :)
Will call on Tuesday

:)
Title: Re: ***WARNING*** tiny brain alert!!
Post by: SilverGems89 on January 02, 2011, 04:58:44 PM
i leave mine for about 3 and a half to 4 hours, i usually stick my hand to the bottom and if its still warm leave them a bit longer, if not i whip em out, im terribly impatient but i havent lost any doing it this way!
Title: Re: ***WARNING*** tiny brain alert!!
Post by: Redhotsal on January 02, 2011, 05:09:55 PM
If your kiln is totally dead your first port of call will be to check the fuse. You only need a screwdriver to do this and you can always swap a fuse from something that you know works - maybe the kettle?, but mind you choose something that has the same amp rating, which I imagine will be 13A for a kiln.

Leaving your beads in annealing bubbles long after they have cooled to room temperature won't make any difference. To be honest - they'll probably be cool after about half an hour but it certainly doesn't hurt to leave them in for longer. Annealing bubbles do NOT anneal beads they just slow down the rate of cooling sufficiently to stop most beads from cracking.
Title: Re: ***WARNING*** tiny brain alert!!
Post by: The Tartan Trout on January 02, 2011, 05:26:35 PM
Quote from: Redhotsal on January 02, 2011, 05:09:55 PM
If your kiln is totally dead your first port of call will be to check the fuse. You only need a screwdriver to do this and you can always swap a fuse from something that you know works - maybe the kettle?, but mind you choose something that has the same amp rating, which I imagine will be 13A for a kiln.

Leaving your beads in annealing bubbles long after they have cooled to room temperature won't make any difference. To be honest - they'll probably be cool after about half an hour but it certainly doesn't hurt to leave them in for longer. Annealing bubbles do NOT anneal beads they just slow down the rate of cooling sufficiently to stop most beads from cracking.

Fuses all checked and in working order...so its not that. I know they wont be annealed I just didnt want my first batch of 'sweetcorn' all cracking :(
It just means by the time I do get it sorted its going to be a huge batch to anneal :)

;D ;D