Hi folks. Just fired up the torch for the first time and still feeling sick (from nerves you understand!). Just wanted to check what pressure the regulator should be set at (it's the oxycon kit with all the tubes etc fitted to the torch which is the Nortel Minor torch from Martin). The torch instructions talk about 6psi but the regulator is in bar (up to 4 I think), it is the big black tap thingy. I have done a search on here for info but am still not completely sure. I think we had it on full blast when we lit it this first time, but don't think we need it that high. Thanks as ever for your help. :)
I have mine set to 5 :)
Thanks Lesley, but is that BAR or PSI, the regulator goes up to 4 bar max? I believe (from reading posts on here on the subject) that the regulator would have been preset by Martin, but of course clever clogs here didn't realise that and fiddled with it so now I don't know what he set it at! I am not going to bead today as I didn't turn on the kiln this morning and its a bit late now as I don't want it going all night at the mo (bit nervous about leaving it on all night).
psi ... my reg is a bar 4 one too :)
Turn the regulator all the way on then back a quarter turn.
If your torch doesn't light, you've turned it all the way off instead.
Thanks Collette will try this tomorrow when I have plucked up the courage to turn it on again. My OH normally knows about gas type things (he brews his own beer and uses a butane burner to boil up his mixtures), so I think there will be alot of 'Honey, help me!' going on. I know once I get going it will be fine, but have been so used to torching at Manda's where it is alrealy set up and safe, that doing it at home is sooooooo nerve racking! Typical newbie! :) Happy New Year. :)
hehe... it'll soon become second nature to you :)
i screw mine all the way down then up a few turns ...i think ...???
which ever mark it so you know where it should be next time ...but i dont generally fiddle with it once its set ....
dont be scared .....the first couple of sessions are a leaning curve i know ..but soon it will all come good