Last week I did some pieces in my kiln. I am still learning how my kiln works and it's hot spots. Some pieces fused more than I had planned and others not really as much.
In particular I did what I hoped would be a pair of earrings with diachroic on purple. On one the diachroic has fused right in (so it spreads and becomes diffused by the top layer) on the other it has remained on top (a very clear dots pattern no diffusion). Now clealry they do not match.
Has anyone ever refused a piece? Wondered if I did that might get the diachroic to move further into the piece and diffuse so they might match.
Marie
theres no harm in refusing at all, the result may be different from the other
re-fuse. it might sort it out if you're after a full fuse
Yep - I have refused. My kiln fuses unevenly and makes me swear at it occasionally :-\
I sometimes refuse, but IMHO I'd suggest that you keep a close eye on it as the glass may also spread out a little and you could potentially lose the shape if you let the heat creep up too much. Probably not too much of a concern if you have a digital controller - but if you don't you could end up with odd shapes. Having said that, you should definitely give it a go!
Fingers crossed for you :)
I occasionally refuse.... but most of the time I'm just easy..... Haha Haha Haha
:-[ Sorry - I'll get my coat now :-[
I liked it Staceyemma ;)
;D ;D ;D ;D ;D ;D
lol.... just how did Tan or Les miss that one
Quote from: stacyemma on June 04, 2007, 08:39:10 AM
I occasionally refuse.... but most of the time I'm just easy..... Haha Haha Haha
:-[ Sorry - I'll get my coat now :-[
Oh you beauty......
never refuse to re fuse ;) or refuse to refuse..or just say yes!!
Hehehe - sounds like a good motto to me :P
Quote from: littlegiggles on June 04, 2007, 10:17:00 AM
lol.... just how did Tan or Les miss that one
Bu**er !!!! I take my eye off the ball for 2 minutes and see what happens ???
;D ;D
How about when you fuse something and the bottom layer spreads and the top layer just sits there? Cut off the extra somehow or refuse to try and get top to spread, or act like that is what you meant to happen?
That's never happened to me ??? Do you cut the top piece slightly larger than the bottom/other layers? I try to do that and then it kinds of 'wraps' around the rest as they fuse
Quote from: Evadark on June 05, 2007, 06:19:01 AM
How about when you fuse something and the bottom layer spreads and the top layer just sits there? Cut off the extra somehow or refuse to try and get top to spread, or act like that is what you meant to happen?
Turn it over and refuse it, or grind it and fire polish?
That happened to me before I started to cut a slightly larger layer for the top.
I tried grinding the sides and re-fusing twice - one time it worked fine on the shape but it did leave very fine lines along the side where it had been ground - the second time I used a finer grinding bit and washed the glass thoroughly before re-fusing and that seemed to do the trick.
I try to always allow for this spread now. There are some useful notes available from Bullseye on this topic - in the technotes section of their website - give me a shout if you need the link and I'll go find it for you. It helped me tremendously!