Hi all,
I wondered if anyone could please advise me on which colour to use? A lady I've just made a red and black necklace for had now asked for an electric blue, black and silver one as well. Whic 104 coe electric blue glass woud you recommend for a vibrant colour? (I'm on a minor). Thanks. ;)
Mand x
CIM pulsar is a lovely transparent electric blue? Or you could try encasing a white core with trans cobalt?
I find pulsar the same as eff dk turquoise trans. some days the effetre seems to pit less than the pulsar. some days it does not!
CIM electric avenue I like lots.
Quote from: MadelineBunyan on December 10, 2010, 02:27:54 PM
CIM electric avenue I like lots.
I was just going to suggest that one!
Quote from: GlassOcean on December 10, 2010, 02:25:13 PM
CIM pulsar is a lovely transparent electric blue? Or you could try encasing a white core with trans cobalt?
I agree re: Pulsar..... its a lovely blue...
Here's a bracelet that I made with it last week.
(http://i262.photobucket.com/albums/ii90/Fruddster/IMGP6988.jpg)
I was going to suggest the Effetre dk aqua too
i'd rock down to electric avenue too ::)
plus 35% off in the tuffnells sale! good times!x
Hmm, I think I may have some dark aqua already .... although I could get me some electric avenue and/ or pulsar. Oh I'm torn, what to do? (Well it's daft asking you lot - you will all just say BUY BOTH!) :D ;D
Well there is a hooge sale on at the moment and it is nearly Christmas and I suspect you could do with a little treat and the sale is so big the money you are saving means you are spending nothing at all really so you could buy more glass and spend even less than nothing......okay? :D
I was just going to say...35% of CIM and freepost...of course buy both! the only problem is what else might happen to fall into your basket!
Yup, bought a few other colours too. BARGAIN! ;D
CIM electric avenue or ming.
This blue is the perfect transparent electric blue. Martin used to sell it by the rod but I can't see it now.
http://www.frantzartglass.com/index.php?main_page=product_info&cPath=79_108_216_142&products_id=3183
Kazx