aurea has stopped doing its shine thing ??? .....not had a problem with it before ...
i read through previous posts and this one came up ..... (it suggested i started a new thead as was a bit old but if a mod wants to add it to the end of this thread feel free )
http://www.frit-happens.co.uk/forum/index.php?topic=21588.0
lee suggests a '' foreign object'' coud cause a change
the only thing changed is the new bead rack ....could this have caused the change in atmosphere in the kiln ?.....and will carbon /charcoal put it back to how it was ?
I've successfully had shiny Triton since adding the bead rack to my Cube, but it wouldn't hurt to try the carbon thingy I suppose.
Take the bead rack out and test your theory. :)
Personally I've never used a bead rack in my kiln, I might be missing out but I haven't noticed ;D