I have made my first button using the two pick mandrell,m I don't seem to be able to get it off the mandrell....any ideas please.
I had the same problem and had to take, er, drastic measures to get the button off of the mandrel. I double dipped the next time and it came off easily.
perseverance and a lot of wiggling!! - Sometimes they are a problem, funny enough they seem to get easier the more you use them
Thanks, I will double dip next time.
Double dip, then soak in water, grip just behind the button with pliers and do the very gentle wiggle thing - hold the button in a damp cloth if you need to.
If all else fails, send it to me - I haven't lost one yet ;D