This might sound daft but I'm totally new to lampworking and very scared of anything that might go bang! I bought an oxycon kit from tuffnells, hubby connected it all up and I have a fire blanket just in case (I also have a bowl of water!). I have spent the week making beads now the propane cylinder seems a bit light so soon enough it will run out.
My knowledge is very limited in that I just read the book 'passing the flame' and Martin Tuffnell showed me how to light the torch at the show. I remember reading 'POOP' so in my mind its not good to leave the oxygen only with a flame....However I realise I have no idea whatsoever what will happen if I'm working away and the propane runs out leaving the oxygen only on (breaking the POOP rule) What will happen? Does the flame just go out, does oxygen burn on its own?
Any help would be appreciated
Thanks
Helen
Your flame will get lower and lower and simply go out. All you need to do is turn everything off as normal, turn off the bottle tightly then disconnect it.
hello helen! (from another another helen...there are a few of us on here! ;) )
no need to worry, your flame will get smaller and smaller and then go out! the oxygen will just come through the torch like air, not burning when there is no propane, so just turn off the oxycon, turn off the gas at the tank and go out and get a new one as soon as you can! ;D
hope that helps my dear, hope it makes sense!
Have fun! x
as julie says the flame runs out of steam , gets lower and goes out..... as mine did this morning.
i have 6 kg propane and it lasts me months so you shouldnt be running out just yet ;)
sandy
Just as you're making the best bead ever at the point that you're not quiet happy but you know this is a super bead the flame will slowly dwindle to nothing - happens every time.............. ::)
Thank you all - I'm such a coward but not knowing was playong on my mind.
I got the six kilo tank and so far I have done about 15 one hour stints max so maybe there is more gas left than I think, Julie, you say 6kg lasts months, do you think my 15 hours is not near the end yet? I should have weighed the thing when we got it full so I could estimate whats left but we just got a new glass bathroom scales and I just didnt dare!
Thanks again everyone
I get the 3.5 kilo tank and even mine lasts a good couple of months torching maybe 6-8 hours a week.
You'll get waaaaay more than 15 hours out of a 6kg tank!
Brilliant! I can have a good go tomorrow see if I can ever get raised dots right!
Thanks again
Helen
Helen, its not a daft question if you don't know the consequences, you are right to be wary of propane, its that respect that will always keep you safe. I write the date on the top of mine when I first start them and it gives me a rough idea how long one lasts me.
If you are really concerned I think there are stick on gauges that attach to the side of the tank that will tell you how low it is. I can't tell you where to get them but I'm sure I remember Princess Pink telling us about them a while ago
Quote from: Tan on November 20, 2010, 08:56:59 PM
I write the date on the top of mine when I first start them and it gives me a rough idea how long one lasts me.
That is such a flippin' fab idea! :D
Sometimes...........and its very rare............I amaze myself at my own genius, its quickly tempered by me doing something extremely stoopid though :D
A big tank lasts me about a year and thats with some pretty heavy hammering as well.
Quote from: Enchanted Cobwebs on November 20, 2010, 05:41:29 PM
I have a fire blanket just in case (I also have a bowl of water)
You should have a fire extinguisher as well, you just never know when/if you will need it (I set fire to my fingernails today ::) :) - not that I needed to use the fire extinguisher!!, but things could get out of control...)
You will know when you are running out of propane - it's not something that suddenly happens - usually occurs over a few minutes.
First sign will be that you flame will get more "pointy" than normal. If you turn your propane down slightly on a normal flame you will see this. You'll find yourself thinking "oh, the flame looks as if there isn't enough propane" and you'll naturally turn up the propane knob to compensate. This will happen a couple of times until you have no more propane to turn up and then the flame will just get impossibly small.
Turn the torch off as normal and change your propane.
As others have said, you're unlikely to have run out yet. An easier way to tell if you're coming near the end of the bottle is that you don't get a "psst" sound when you open the valve. As the propane runs out the gas pressure drops and so you can open the knurled knob on top of the cylinder without feeling the pressure.
Even if you ran out of propane and left your oxycon on you wouldn't get anything bad happening. The pressure on an oxycon is much lower than on tanked oxygen so you really won't get a flashback or anything nasty happening. The extra oxygen will just blow out the remaining propane (which will be at a low pressure anyway) and you'll just get oxygen flowing through the torch. No worries.
Quote from: ARBeads on November 20, 2010, 05:52:04 PM
Just as you're making the best bead ever at the point that you're not quiet happy but you know this is a super bead the flame will slowly dwindle to nothing - happens every time.............. ::)
Nil desperandum, just garage the super bead, anneal as normal, leave in kiln until you get more propane. Set kiln off again till it reaches annealing temperature, leave for a few minutes until the bead is thoroughly heated through ( the bigger the bead the longer you leave it), take out and finish reworking it until you are happy. Garage again. I do this with a large bead, say a goddess, if I get tired half way through.
Quote from: Tan on November 20, 2010, 08:56:59 PM
I write the date on the top of mine when I first start them and it gives me a rough idea how long one lasts me.
If you are really concerned I think there are stick on gauges that attach to the side of the tank that will tell you how low it is. I can't tell you where to get them but I'm sure I remember Princess Pink telling us about them a while ago
Good idea about noting the date.
You can get guages from Kleeneze for £6, but they are pretty useless. I sent mine back, it kept falling off, they don't fit the 3kg cylinder and on the 6kg it thought I had run out about 15 hours before I had. If there is a decent guage that actually works can someone enlighten me?
I know when my gas is running out, I find I'm working about 2cms from the end of my HH, peering at the flame and cursing because the glass is taking an age to melt. I find when the gas is really low, if I put the cylinder (if you can lift it) in a bowl of hot water I'll get another hour or so out of it. Doesn't help my shedio is like a fridge at the moment; didn't do science but something to do with gas is more liquid in the cold?