I'm struggling a bit !

Martin very kindly sent me a bead rack for inside my kiln, but I've found that once its full, it takes about 20 beads, its very difficult to add more, so I have gone back to the old method of just placing them on the floor on my fibre mat.

But I'm having difficulty moving them over, through my bead door.

Once I have 5 or 6 in there, I use my tongs to try and move over the ones that have been in there a while, so that there is space for the new ones, but they just go everywhere and I find myself bent over, tongs in hand, trying hard not to burn myself, peering through the bead door, trying to move them all over enough so that I can shut the door!  I know that people refer to "stacking them up" once they have been in there a while, to make room for new ones, but I cant seem to do this, when I grip the mandrels with my tongs, even one by one, they slip and slide all over the place and then I have to try and re-arrange them as best I can enough to get the door shut and it is really doing my head in!!  Sometimes I can be fannying about for over a minute, by which time the temp in the kiln has dropped almost 10 degrees!

What am I doing wrong here??
Title: Re: Stacking Beads in the Kiln
Post by: Kalorlo on November 20, 2010, 03:24:36 PM
 ??? What kind of kiln did you get? My mandrels stick out of my bead door, so the ends are cool enough to move normally.
Title: Re: Stacking Beads in the Kiln
Post by: MadelineBunyan on November 20, 2010, 03:26:27 PM
try using a leather glove (gardening type, or heavier duty ones, squires do some http://www.squirestools.com/) to move around your mandrels, I can't do it with a tool either!

also, I tend to move them around a bit, reclose the door, count to ten, then have another go, then I don't lose too much temperature.

I have a strip of fibre blanket that goes across the inside the front edge of the kiln, this keeps the smaller beads off the kiln floor.

I recently made myself a rack out of stainless steel mesh, but I'm finding it annoying from time to time. whats nice about it is, that because its a mesh, you can stick the ends of mandrels in anywhere in it, so bigger beads can have more room around them.

I have an sc2, so the mandrel ends stick out, but I cant touch them, too hot! especially BHB ones!
Title: Re: Stacking Beads in the Kiln
Post by: Fruddy on November 20, 2010, 04:02:09 PM
Quote from: Kalorlo on November 20, 2010, 03:24:36 PM
??? What kind of kiln did you get? My mandrels stick out of my bead door, so the ends are cool enough to move normally.

I've got a Prometheus, its very similar externally to an SC2.

Is it not essential then to have your bead door fully closed??
Title: Re: Stacking Beads in the Kiln
Post by: Blue Box Studio on November 20, 2010, 04:07:48 PM
The bead door on my SC2 doesn't fully close when I have mandrels sticking out.  I put the manderels in my bead rack, then when I run out of room just pile them all up together on one side, making room for more.  By the time you are ready to do that they shouldn't be sticky if they touch.  A lot of my mandrels are 9" which I find a bit short for manoevering around through the door so the gardening gloves tip is a good one - off to the shed now.  I much prefer batch annealing, I get in less of a muddle.
Title: Re: Stacking Beads in the Kiln
Post by: Margram on November 20, 2010, 04:35:48 PM
You're gonna laugh - but I put my hand in an old sock to move the mandrels in my SC3!!! ;D You can just plonk the beads on top of each other after they have been in there a few minutes, unless they are rubino which can be sticky...
Title: Re: Stacking Beads in the Kiln
Post by: Fruddy on November 20, 2010, 05:03:51 PM
Quote from: Margram on November 20, 2010, 04:35:48 PM
You're gonna laugh - but I put my hand in an old sock to move the mandrels in my SC3!!! ;D You can just plonk the beads on top of each other after they have been in there a few minutes, unless they are rubino which can be sticky...

Ah!  A sock!!  What a fab idea!!  I have two odd old hiking socks which are thick would be just the ticket!!

Cheers chuck!
Title: Re: Stacking Beads in the Kiln
Post by: dangerousbead on November 20, 2010, 05:10:55 PM
Mine stick out too, and They're cool enough to handle. I didn't know I could pile them up though. Good tip. Thanks
Title: Re: Stacking Beads in the Kiln
Post by: Blue Box Studio on November 20, 2010, 05:22:37 PM
Quote from: dangerousbead on November 20, 2010, 05:10:55 PM
I didn't know I could pile them up though. Good tip. Thanks

Neither did I until I accidently moved on in class, panicked thinking I'd ruined someone else's bead and was then enlightened.

Didn't know about Rubino, so will bear that in mind - not that I have much of it to use anyway.
Title: Re: Stacking Beads in the Kiln
Post by: Lush! on November 20, 2010, 05:55:22 PM
A bead door is designed to be left slightly open, with all the mandrels sticking out.  You're likely to injure yourself if you're pushing the mandrels all the way in then rearranging them!

The bead door is open in this photo to show the rack, but you can see how they're all piled up (over-stuffed actually!).

(http://farm4.static.flickr.com/3218/2757601371_bf65aeb242.jpg) (http://www.flickr.com/photos/lushlampwork/2757601371/)
A kilnful of fresh beads! (http://www.flickr.com/photos/lushlampwork/2757601371/) by LushLampwork (http://www.flickr.com/people/lushlampwork/), on Flickr
Title: Re: Stacking Beads in the Kiln
Post by: MadelineBunyan on November 20, 2010, 06:30:11 PM
I love it when my kiln is stuffed full like that! seeing all those mandrels sticking out makes me happy, cause I know theres something pretty on the other end! (of at least some of them anyway!)

sadly not often at the moment. mojo has gone awol. hoping for some this evening, though I would be happy with a single layer!
Title: Re: Stacking Beads in the Kiln
Post by: mel on November 23, 2010, 04:48:36 PM
I have a paragon Caldera with a bead door. I used to shove my beads in and leave the mandrels sticking out, but found that quite often the bigger beads would crack even after annealing. What I do now is to put them in first so they arent touching anything in case the surface is still tacky, then after every few beads made I move them over to one side (using pliers), and if they touch it doesnt matter so much. When I've finished at the torch, I get my paddle and push all the mandrel ends so that the bead door just about shuts, this also shoves the mandrel holder and beads towards the back of the kiln. I count this as the starting point of the soaking time as even the first beads in may have been sitting at slightly lower than annealing temp due to heat loss down the mandrel.

If the mandrels are getting too hot to touch (like mine do), then it means that heat is leaving your bead and travelling along the mandrel and I sort of guessed this accounted for my cracked beads on occasions.

This may be a lot of old tosh, but it works for me.
Title: Re: Stacking Beads in the Kiln
Post by: Billie on November 23, 2010, 04:55:28 PM
I found that bead rack useless...  :-\  I have a caldera with bead collar too, and I got a piece of stainless steel mesh from the DIY shop for about 4€, trimmed it so it sits inside the kiln, and bent it into a U shape, but with the front shorter than the back (so it's maybe like and L with a lip at the front).  I can then put the mandrels in, and layer them.  I'd take a picture, but the kiln is on at the mo...
Title: Re: Stacking Beads in the Kiln
Post by: mel on November 25, 2010, 01:55:51 PM
That sounds interesting Billie, moving hot beads around is a bit of a faff and I'd rather not have to. A photo would be fab if you have the time/inclination.
Title: Re: Stacking Beads in the Kiln
Post by: Billie on November 25, 2010, 02:23:43 PM
Quote from: Helen P on January 21, 2007, 01:46:39 PM
I got the steel mesh from B+Q, and cut and bent it to fit inside my kiln.? There are many other ways of doing this, these are just the ways I've tried.


Here are the kebab images - 1. kiln shelf post set up:
(http://i154.photobucket.com/albums/s250/BeadyBugs/FH%20images/KebabstandL.jpg)


2. Wire mesh cradle set up:
(http://i154.photobucket.com/albums/s250/BeadyBugs/FH%20images/MeshmandrelstandL.jpg)

If anyone has any other suggestions or schedules, please feel free to add them.

Cheers! ;D? HP x

Got the idea from this thread http://www.frit-happens.co.uk/forum/index.php?topic=859.60

Helen has hers in sideways, and the two sides are equal height.  My mesh is turned around so it is higher at the back, and has a slight lip at the front.  HTH.  Have a poorly child at home, and escaping to take photo's while we have some light is proving impossible  ::)
Title: Re: Stacking Beads in the Kiln
Post by: dangerousbead on November 25, 2010, 03:41:13 PM
Slightly off topic but I'm pleased to see other people's kilns have rusty stains and rust looking fittings. I was quite dismayed when this happened on it's first run, my pure white interior looking like an old loo.  >:(