Frit-Happens !

Fusing and Stained Glass Tips and FAQ's => Fusing Tips and FAQ's => Topic started by: Lucas on November 20, 2010, 11:50:57 AM

Title: Kiln wash or kiln paper
Post by: Lucas on November 20, 2010, 11:50:57 AM
Hi all,
I have a kiln coming on Monday from warm glass( ;D ), and have done fusing on an evening class but tend to use kiln paper.  Now I'll be doing more I thought I might need to look at kiln wash for financial reasons, but not sure how it works... ???
Are you supposed to use kiln wash on shelves even if you use paper too, or is it one or the other?  I hope to do some slumping and using moulds later, when I get the hang of things (and can afford the moulds! ::)), and I know I'll need wash for that, but for the time being will be concentrating on tiles/coasters/anything else I can think of!
Any recommendation of specific brands or suppliers for kiln wash, or do you think I should just stick with paper?  And what about the clean up (of paper or wash) - I assume there is some(or should be some!) but to be honest we skimp at the evening class, no dust masks or anything, just wash the pieces off in the sink!
Any info/advice/recommendations welcome!
L
Title: Re: Kiln wash or kiln paper
Post by: Margram on November 20, 2010, 12:07:03 PM
Quite a lot of info on this thread: http://www.frit-happens.co.uk/forum/index.php?topic=22629.0
Good luck! :)
Title: Re: Kiln wash or kiln paper
Post by: Blue Box Studio on November 20, 2010, 04:10:23 PM
Warm Glass sold me kiln paper and siad it was easier to use than kiln wash.  I got it because a friend uses my kiln for fusing small dichro pieces and she has always used kiln paper in her classes.  Don't think it was horrendously expensive and I can get 4 pieces for my SC2 out of a big sheet (or was it 6?) but I guess if you were doing a lot kiln wash would be cheaper.
Title: Re: Kiln wash or kiln paper
Post by: Zeldazog on November 20, 2010, 05:45:03 PM
Hi Lucas

As you'll probably gather from the other thread, kiln wash or paper is a matter of personal preference.  Yes, paper is much much easier, but as I wrote in the other thread, works out something like 10 times more expensive.  Personally I can't justify that cost - if I was fusing occasionally, then I would probably not worry.

If you use thin fire, or ceramic fibre paper, you won't need to wash the shelf. But if you use thin fire, you will need to hoover out the kiln each time and use a new sheet.  I have tried CF paper, which with care, and not moved, will last more than one firing, but I personally didn't like the texture it left.

I don't know what wash you use at your evening class, but it should not really be washed down the sink. 

I usually use Bullseye shelf primer, and it won't wash off anyway!  I used to remove it with a green scourer, wearing a dust mask, but recently found out that a metal paint scraper does a much better and quick job of getting it off, creating far less dust - but it goes into the waste bin, not down the sink.  Ideally, you should also be wearing a dust mask when you mix it up too.  A haik brush is very useful for applying the kiln wash.

Warm Glass have started selling a new shelf primer which I think *does* wash off, so I might try that, although I'd still want to research a bit more before sticking that product down the drain....




Title: Re: Kiln wash or kiln paper
Post by: awrylemming on November 20, 2010, 06:13:22 PM
I bought some kiln paper which I was going to use for fusing, but have come to the conclusion that my disability precludes this - so the paper is now defunct, and I have a huge tub of kiln wash anyway.  It's yours if you want it, and already in a tube, so just needs an addy and postage.  I'll pick up the postage tho, it won't be much.
Title: Re: Kiln wash or kiln paper
Post by: ♥♥Tan♥♥ on November 20, 2010, 06:40:54 PM
I will if he doesn't Sue, I'm just about to run out! ;D
Title: Re: Kiln wash or kiln paper
Post by: awrylemming on November 20, 2010, 08:45:17 PM
Whoever pm's me first is more than welcome to it. :)
Title: Re: Kiln wash or kiln paper
Post by: Lucas on November 20, 2010, 09:13:29 PM
Have PM'd you, but don't know if I won the race!
And to clear up any confusion, I'm not a man, just have a name which sounds like I should be!!
Lucas
Title: Re: Kiln wash or kiln paper
Post by: Lucas on November 20, 2010, 09:20:41 PM
Thought I should clarify - we use thinfire paper at the class, so it's the dust left on the fused pieces which gets washed down the sink, not sure if I've ever seen a vacuum anywhere near the kiln though...
Might start off with paper til I get a bit more experienced, think there's going to be a steep enough learning curve as it is! 
Thanks for the info folks!
Lucas
Title: Re: Kiln wash or kiln paper
Post by: Zeldazog on November 20, 2010, 10:06:18 PM
Honestly Lucas, kiln wash is easy peasy to use.  Mix with water, brush on several coats (in different directions). 

I then usually fire the shelf up to 200 degrees, take it out, give a rub over with a piece of kitchen towel (or my hand), perfectly smooth shelf that will usually last more than one firing.

Advice from Bullseye regarding thin fire: 
http://www.warm-glass.co.uk/Downloads/Public/Products/Safety%20Files/Bullseye%20Thinfire.pdf (http://www.warm-glass.co.uk/Downloads/Public/Products/Safety%20Files/Bullseye%20Thinfire.pdf)


Title: Re: Kiln wash or kiln paper
Post by: julieHB on November 21, 2010, 09:43:15 AM
I don't do much fusing these days, but I might just have to treat myself to a pot of kiln wash  :)
Title: Re: Kiln wash or kiln paper
Post by: Lucas on November 21, 2010, 07:19:28 PM
So how do you know when you need to re-coat it, if sometimes it lasts more than one firing?  Would it be blatantly obvious, or might I not realise and wreck everything?  Can you just kind of 'top up' the kiln wash on the shelf, or do you have to scrape it all off (with a paint scraper into the bin - I was following!) and start again every time?
Thanks for the info and help, I don't want to ruin everything before I manage to get anywhere!
L
Title: Re: Kiln wash or kiln paper
Post by: Zeldazog on November 21, 2010, 09:37:40 PM
Sometimes, the shelf looks the same - well it will be creamy colour, when it was probably a pinkish shade when it first went in.

Sometimes there will be darker shaded areas where your glass was - if there are no loose flakes, I don't worry.  Sometimes there will be just lines where the edges of pieces have come away.  Sometimes, depending on placement of these, and the size of the next batch for firing (And what temperature I am going to) I will just work around them.

And other times, whole areas of kiln wash will come away.  Basically, if it's coming off, its coming off - it WILL be obvious, as the wash is different colour to the shelf - it doesn't just get thinner and thinner.  It's either there, or it's not, so don't worry, you will be able to tell I am sure.

I *have* re-coated over a shelf where a bit has come away - and still do occasionally - but only on small pieces - and I did this before I discovered the paint scraper method.  However, when I tried to fuse a plate on a shelf I had re-coated over a flaky bit, I had problems - the shelf is then uneven, and trapping air underneath - so honestly, it's not really worth it - this doesn't tend to be an issue with small pendant sizes, as they rarely cover the whole area that might have flaked.  Hope this is making sense!

I can only say this about Bullseye Primer, as I haven't used any other sort myself.  The batt wash at college was the same though, but I can't say for sure what brand it was.

Title: Re: Kiln wash or kiln paper
Post by: julieHB on November 21, 2010, 10:35:04 PM
Well, I have ordered a small bottle of Primo, and am excited to try it out - the fact that it supposedly is easy to clean off both glass, kiln shelf and moulds is a huge selling point  :) Will report how I get on!
Title: Re: Kiln wash or kiln paper
Post by: Zeldazog on November 21, 2010, 10:41:41 PM
I think I am going to try and small pot next time I place an order, then whichever I prefer I will buy a big tub, as I am now getting through a lot more!

But do let us know Julie, it did appeal to me too!
Title: Re: Kiln wash or kiln paper
Post by: Pat from Canvey on November 22, 2010, 09:17:16 AM
I used to use a haik brush for my shelves but you can get an interesting finish if you use one of those small paint rollers, the foam kind.
Title: Re: Kiln wash or kiln paper
Post by: Warm Glass UK on November 22, 2010, 09:54:46 AM
Here's the link to our document on kiln wash application/reapplication if it helps :

http://www.warm-glass.co.uk/Downloads/Public/Products/Tools/Using%20Shelf%20Primer.pdf

Thanks, Pippa
Title: Re: Kiln wash or kiln paper
Post by: ♥♥Tan♥♥ on November 22, 2010, 02:01:31 PM
Thankyou for taking the time to post that Pippa, its valuable info!
Title: Re: Kiln wash or kiln paper
Post by: Grody on December 02, 2010, 03:17:31 PM
Despite being a Yorkshireman (definition: like a Scotsman, but with the boundless generosity removed), I feel life is too short for kiln wash.

The price of the BE paper from Warm Glass is attractive (unlike their shipping charges) and I don't need any more faffy processes to deal with when all I want to do is fuse! Been making cufflinks in quantity for the last few months (500 pairs+) and the paper has been a godsend. Yes, you may save a bit of dosh but your sanity has a value too.

Just my take on it.
Title: Re: Kiln wash or kiln paper
Post by: Zeldazog on December 02, 2010, 04:27:51 PM
Fair comment Grody, although I have to say it really doesn't take that long to coat a shelf, probably less than a couple of minutes, usually lasts two or three firings, and since discovering the metal scraper method of cleaning 'tis a doddle to clean off too.

Title: Re: Kiln wash or kiln paper
Post by: Zeldazog on December 02, 2010, 04:28:07 PM
Incidentally, Warm Glass have free shipping today..... 
Title: Re: Kiln wash or kiln paper
Post by: Sarah A on February 19, 2011, 09:02:04 PM
Glad I stumbled across this thread.  I have used kiln paper since I got my kiln as the lady I bought it off gave me a couple of pieces though when I got my larger kiln decided to try kiln wash as much cheaper but hate taking it off, was using the green scourer so was going back to kiln paper.  Will now try the paint scraper way and see how that goes.  Did anyone try the new kiln wash from warm glass?
Title: Re: Kiln wash or kiln paper
Post by: stuwaudby on February 20, 2011, 11:47:29 AM
First and most important advice is to use a flat shelf. The texture on the back of your pieces is so much smoother and the glass flow is more predictable. We use both paper and wash depending on the piece. We tend to use paper for small pieces where the base layer is whole sheet. Where the base layer is multiple pieces of glass or layered then wash works better. If you will see the back face then wash gives a smoother finish. Dont be put off by wash, its much cleaner to deal with and once the shelf is initially washed is stright forward to top off. We use very thin washto just give a consistent covering. A quick vac brush outside is sufficient to clean it for next time, it rarely gets extra coats.

Main bit of advice is make sure your kiln shelf if lifted off the base of the kiln. It will then get a more consistent temperature. Pieces close to the edge of the kiln sometimes get less heat at near the edge. 

Good luck and enjoy the new kiln.
Title: Re: Kiln wash or kiln paper
Post by: Lucas on February 21, 2011, 08:17:15 PM
Hi Sarah,
I have bought a little thing of the new wash (primo or something I think it's called, though this may not be right! ::)) and haven't used it yet - I'm using the ordinary bullseye wash for my shelves (and using a thicker layer than others, but this lasts ages without having to scrape off and recoat, and still leaves a very smooth back). As I just have the one shelf I leave it to dry for at least a day (often two) and have had no problems with bubbles etc from moisture.  I am planning to use the new wash for moulds, as I can see me breaking them while trying to use the paint scraper method to get old wash off, even though I know you don't have to do this often as the temp doesn't go so high - once would be enough for me to wreck it! 
How about you - have you been using the new wash off primer or are you researching before you buy? 
What kind of stuff are you making?  Many of the lovely people on here are bead orientated (and they are just gorgeous - check out the gallery!) ... (I mean the beads, but I'm sure the artists are gorgeous too!! ;D ;D) ... not a lot of fusers who don't do beads!

Lucas
Title: Re: Kiln wash or kiln paper
Post by: Sarah A on February 22, 2011, 09:52:46 AM
Hi Lucas

I haven't got any of the new prima yet as still have loads of the bullseye one yet though it does sound like a good idea for moulds.  Do let me know what you think of it when you have tried it.

And yes the beads on here are gorgeous.  I mainly fuse but got a bead making kit last month and am now slowly getting the bead bug!