I am wondering what colours have Bern used as base colours for silver glasses with best success or interesting results - all I know to use is the standards Ivory or Opal Yellow.
Also opal yellow is so shocky and expensive l, does anyone know a cheap alternative?
Cobalt or Ink Blue are both good..
Effetre Pearl Grey, i use it underneath dots of psyche and get beautiful purple colours!
I love CIM transparent lime green, CIM commando, white and effetre transparent baby blue. I also love black and transparent ambers with lots of the silver glass also.
Pearl grey I think Iv got that, this could get my mojo back Iv been off torch feels like I hit a wall or something ;)
Quote from: helbels on November 08, 2010, 09:59:51 PM
Cobalt or Ink Blue are both good..
which silver glasses do you use these with Helen? i've never tried either (under silver glass anyway)!
okay white is great under ekho and kalypso, and i reckon it'll work good under terra 2 as well.
i like dark lavender, pale amethyst and clear under clio
under aurae i use clear, black, pink lady/rubino/gold ruby bright, also gold violet is amazing with it.
psyche-ivory, opal yellow, porcelain, black, cobalt trans
triton-cobalt trans, black, lapis (amazing!!)
hope that give you some ideas :)
Wonderful thanks well I'd better fix my extraction sharpish. I Need a kick up the Bum lol
go for the handpulled colours, they always work well with silverglass.
CIM Dirty Martini with Psyche
Eff Red Purple with Psyche
Eff Trans Teal with Aurae and Psyche
Eff 006 clear with Aurae