Frit-Happens !

Lampwork => Common Problems => Topic started by: tredan1973 on November 07, 2010, 08:23:39 PM

Title: Lampwork start up
Post by: tredan1973 on November 07, 2010, 08:23:39 PM
 ???

Can anyone spare their thoughts on a lampwork start up for me, a newbie :

I have a shed,but that is far as i have got.  A few questions:

basic kit? needs and musts
I know ventilation but can anyone advise me regards what sort (hubbie is not of a DIY nature) cooker fan surfice or anyone know of better idea?

I have surfed, extensively lol and have been recommended Martin from Tuffnells which i will do as i have my eye on kit already ;)

I am more concerned over shed? would i need to insulate it? is it suitable in wooden shed? its 8x6?

If anyone can help and advise i would be very, very grateful.
Title: Re: Lampwork start up
Post by: sparrow on November 07, 2010, 08:30:46 PM
Hi Teresa,

Welcome to the forum. I'm not in a shed, but this thread has lots of useful info in, I think - happy reading!

http://www.frit-happens.co.uk/forum/index.php?topic=21843.0
Title: Re: Lampwork start up
Post by: Blue Box Studio on November 07, 2010, 08:37:39 PM
My cooker hood got fried quite quickly because it was not that far above me due to the sloping roof.  I have a kitchen extractor fan now but need to remember to put it on before I light up, elose the heat explans the finds and they start to rub the plastic casing.  I think something better is called for but funds don't allow at the moment.
Title: Re: Lampwork start up
Post by: ScarletLeonard on November 07, 2010, 08:47:20 PM
I bought a basic kit last year (hubby found one on ebay which was still from martin at tuffnels but mid way between the two on his site.)

I regret not going for at least the Deluxe Plus Kit though after spending a small fortune on Mapp Gas I wish I had jumped right in to the The Ultimate Hot Head Kit so I had all the tools and everything. I certainly don't regret my hothead (though now I am pining for dual fuel)



Title: Re: Lampwork start up
Post by: Lindamay on November 11, 2010, 08:25:32 PM
Hello! I saw a demo of bead making and I am thinking of buying a hothead kit from Tuffnells, but I am a bit worried about the cost of the MAP gas because it seems quite pricey. How long does a canister last? Is it worth my while getting a Bulk Fuel Hot Head Connector Kit?
Thank you in advance for any advice.
Linda May Jones
Title: Re: Lampwork start up
Post by: ScarletLeonard on November 11, 2010, 08:44:51 PM
I found they lasted about 3 hours. Bulk fuel is certainly more economical (I use flogas) I have a 19kg cylinder which I have had since march this year. That cost me £28 and no bottle deposit. The Mapp is about £14 a can.

Title: Re: Lampwork start up
Post by: ♥♥Tan♥♥ on November 11, 2010, 08:55:33 PM
http://www.frit-happens.co.uk/forum/index.php?board=130.0

There you go flower, how to find everything you need to know and welcome to the forum ;D
Title: Re: Lampwork start up
Post by: Lindamay on November 11, 2010, 11:24:55 PM
That's great. Thank you very much for your advice.  :-]

Linda May
Title: Re: Lampwork start up
Post by: jensroom on November 13, 2010, 09:19:40 AM
"I found they lasted about 3 hours"

Hi! I'm new to this - bought the hothead basic kit from Tuffnells's stand at the NEC a week ago. He's asked me to send my torch back in case it's faulty, and he's sending me a replacement, because the MAP gas only lasts 2 hours. Are you sure it's right that yours only lasts 3 hours? Before I bought my kit I asked how long the gas lasts, and he said about 8 hours. Do most people get 8 hours out of theirs?

Thanks

Jen
Title: Re: Lampwork start up
Post by: paintboxcrafts on November 13, 2010, 10:00:32 AM
Hi,
I used to find the main problem with Mapp gas cylinders was that they got cold very quickly, reducing the flow of gas and the making it very hard to melt anything. This would happen after 15 to 20 mins. You could have two cylinders and swap them over. I think some people have come up with novel ways of keeping the cylinder warm, maybe they'll chip in and let you know.
I have no patience so I gave up trying for 2 or 3 years, until I could afford a big girls torch., but lots of people do wonderful things on a hot head with bulk propane.
Cathy
Title: Re: Lampwork start up
Post by: Lotti on November 13, 2010, 10:36:37 AM
Can you get a problem with bulk fuel getting cold too?  Our outbuilding which I am taking over has lots of ventilation! but in turn can be bitterly cold and I was wondering if that would have an effect on the propane. (probably a really silly question as I believe alot of people keep their bulk fuel outside? :)
Title: Re: Lampwork start up
Post by: Fruddy on November 13, 2010, 10:40:40 AM
Quote from: jensroom on November 13, 2010, 09:19:40 AM
"I found they lasted about 3 hours"

Hi! I'm new to this - bought the hothead basic kit from Tuffnells's stand at the NEC a week ago. He's asked me to send my torch back in case it's faulty, and he's sending me a replacement, because the MAP gas only lasts 2 hours. Are you sure it's right that yours only lasts 3 hours? Before I bought my kit I asked how long the gas lasts, and he said about 8 hours. Do most people get 8 hours out of theirs?

Thanks

Jen

I have never used Mapp as went straight onto a Minor and Oxy when I set up at home, but I have heard many people say that they can literally only get about 3 hours out of a can of Mapp.   Apparently the can can also freeze up at the bottom (not sure why).
Title: Re: Lampwork start up
Post by: ★★Terri★★ on November 13, 2010, 11:23:39 AM
Me and the Hot Head have been together for a year, and we are extremely happy ;D

Mapp, for me was a disaster - cylinder getting cold very quickly - hubby standing by with lighter to constantly re-light before the blob of glass got too cold.  Went over to bulk propane early this year - still on same tank.  I made my own conversion kit up, but if you are not confident then buy one from Tuffnels.

Orginal shed was a brick built workshop at our last house - and was all my own space (shared with spiders).  Now I have the corner of an old 6x8 shed ::).  I made a little bench with some scrap timber.  Ventilation - well if it was any more ventilated I'd be outside.  Insulated - dress warmly and wear thermal socks.

I use my hobby ceramics kiln to batch anneal and it works fine - a slow cooker full of vermiculite to cool the beads.

I use a variety of tools - some 'proper' lampworking ones - mashers, hand held marver/paddle thingy and a lentil press.  The rest are an assortment of 'things' I have found - screw drivers, hobby blades/scalpels, tiny little butter knife, metal skewer, a little metal mitre box that is a super rod rest and keeps stringers together, jam jars, tweezers, pliers etc.  I make my own bead release which is super - works a treat and cleans off really easily.

I suppose if I had more momey I could be more 'professional' in my equipment - but what I have works for me ;D
Title: Re: Lampwork start up
Post by: Redhotsal on November 13, 2010, 01:58:51 PM
Quote from: Lotti on November 13, 2010, 10:36:37 AM
Can you get a problem with bulk fuel getting cold too?  Our outbuilding which I am taking over has lots of ventilation! but in turn can be bitterly cold and I was wondering if that would have an effect on the propane. (probably a really silly question as I believe alot of people keep their bulk fuel outside? :)

Lotti,
No you don't get a problem with the bulk cylinder getting too cold. The reason it happens with the small canisters is because the gas is first pumped into the canister under high pressure. The pressure is high enough to liquefy the gas (you can hear it sloshing around when you shake the canister). The canister is fitted with a valve with a very small opening. When the valve is opened, the gas escapes from the container and expands quickly. At the same time, and as a result of this expansion, its temperature drops and this is what causes the canister to cool down.
Because the canister is relatively small it is very easy for the expanding gas to cool the entire canister relatively quickly - and as the temperature of the canister drops, so does the gas pressure.

This doesn't happen on a bulk system because the propane cylinder is a much bigger reservoir of gas - even the smallest 3.9kg won't freeze up in the same way so you can be  confident that you won't have a problem with the flame getting smaller on a bulk system (unless you're about to run out of gas).

It's not so much the ambient temperature that causes the problems (it will have an effect to a small degree, but not so's you'd notice_. Your problem actually comes from the gas that's leaving the canister.
Title: Re: Lampwork start up
Post by: Lotti on November 18, 2010, 01:29:37 PM
Thanks Sal, reassures me.  Also worried about the hot head getting rusty as the outbuilding's windows aren't exactly watertight!  I get the impression though that alot of folks are working in similar conditions so I guess it should be OK.  I suppose if I am not using it for a while I could always undo it from it's clamp and bring it indoors? :)
Title: Re: Lampwork start up
Post by: Redhotsal on November 18, 2010, 01:39:57 PM
It'll be okay - it won't rust as it is made of brass, but it's possible that you may get a spider or something trying to live in it. I've heard of this problem a couple of times - people have experienced a mysterious blockage only to have an unfortunate insect be ejected. Not exactly pleasant!
Title: Re: Lampwork start up
Post by: Lotti on November 18, 2010, 02:59:20 PM
 :o :o ;D ;D ;D  Hopefully it won't be one of those big ones with green fangs that have been in the news!  Once got a mouse in the toaster!

Thanks for your help. :)