I'm really struggling with this.
I've bought some findings and some stringing wire etc., so I thought that I would have a go at making a couple of simple bead sets with a view to making my first bracelet.
However, I'm finding it really difficult to make a set of the same size!
I tried last night to make six simple beads, three black and three red, with a little silvered ivory stringer for interest. How hard can that be, I thought! Bloody hard!
I started trying to remember how many wraps of glass I used, for example 10, but I could never tell when I had completed a wrap on the mandrel, particularly towards the end when the wind of glass got bigger (I use the snail shell technique). I thought that they were all reasonably the same sized, but when I took them out of the kiln this morning they were nowhere near - 2 of them were pretty close, but the other 4 were all different and obviously didn't look anything like a set!
Can anyone give me any advice? I see loads of gorgeous bead sets on here, and they are all identical in size. How do you achieve this?
Sorry Rachel but the simple answer is years of practice :)
It's a bit like cooking - eventually you know just how much of the ingredients you need!
Kazx
Fruddy, that's one of the hardest things to do. You could practice, practice, practice... or alternatively use calipers to try to measure your beads as you make them.
However, the easiest way is to buy a beadroller or two from cgbeads.com - they aren't cheap but worth their weight in gold
- the rounds and donuts are an absolute godsend and make it super easy to get the same size beads.
Helen.
Quote from: Kaz on November 06, 2010, 05:28:19 PM
Sorry Rachel but the simple answer is years of practice :)
It's a bit like cooking - eventually you know just how much of the ingredients you need!
Kazx
I had a sneaking suspicion that this was going to be the answer! :)
You know me......patience is not something that I have in abundance, but I shall persevere....!
I struggled for a few weeks getting my big hole beads precisely round, but have mastered this now, so shall adopt the same approach with the bead sets!
Off to the shed now to put this into practice!
Thanks guys.
Quote from: helbels on November 06, 2010, 05:28:43 PM
Fruddy, that's one of the hardest things to do. You could practice, practice, practice... or alternatively use calipers to try to measure your beads as you make them.
However, the easiest way is to buy a beadroller or two from cgbeads.com - they aren't cheap but worth their weight in gold
- the rounds and donuts are an absolute godsend and make it super easy to get the same size beads.
Helen.
Thanks Helen.
Try twisting a piece of wire into a circle about the size of the beads you want - it gives you the chance to check your bead size as you're making it. But it's taken me a good six months just to be able to produce a few beads of similar size, it is down to practice.
Fruddy, not sure if this will help because I use the counting wraps method but I have heard of people marking off their rods into specified lengths and then only melting up to that point. Following a similar method I have read of people cutting the rods into exact lengths and attaching them to a clear rod and only melting up to the clear.
Does any of that make sense? It does in my head
I went through a while wondering this and I ended up making a load of plain white beads in different sizes. (all the rough sizes that I liked to work to.)
I then wrote on them how many wraps they were with a small perm marker.
When I went to make a set of beads I took out the size I wanted and put it in between my fingers on the mandrel
I checked the bead I was making to the dummy and it helped don't use the dummies any more.
Quote from: Tan on November 06, 2010, 05:37:37 PM
Fruddy, not sure if this will help because I use the counting wraps method but I have heard of people marking off their rods into specified lengths and then only melting up to that point. Following a similar method I have read of people cutting the rods into exact lengths and attaching them to a clear rod and only melting up to the clear.
Does any of that make sense? It does in my head
It makes perfect sense Tan, and is a bloody good idea! I shall try that! Thankyou!
I have found it just takes judgement that only comes through practice. My mum (jayspangles) is always asking how I get mine about the same size without always using a beadroller and I just can't explain it - I guess they aren't all perfectly the same size but near enough and unless they are going to be threaded in close quarters then as long as they are within perhaps 2mm then I'm more than happy. The beadrollers are great though - and dead easy to use. But yes practice practice practice is my reckoning.
I'm still at ppp stage. But have found that if I slip a bead of the size I am aiming for on to the other end of the mandrel, it is then there by my fingers as a guide. I can try and make my new bead to that size. (The 'guide' bead does not move right up the mandrel because of the bead release - make sure it was made on the same size mandrel as you are using.)
As each bead is made, I slip the 'guide' bead off and on to the next mandrel. A little fiddly I guess, but I find it helps me!
That sounds a great idea thanks
My beads are getting there for uniformity like I can get 7 out of 8 correct and probably because I am sick of the combination, number 8 comes out a totally different size.
Will try this as it sounds a great idea
Thanks
I started by making a graduated set of beads I liked the sizes of, and then left them lying around my bench as reference beads which I could hold against the new bead for a visual reference.
Really is a PPP thing - now I do most of them without really thinking about it, though I think you get used to the weight of bead as your forming the glasss.
Have fun practising x
I just make lots and then pick the best for the set :) If they vary in size, line them up so they graduate, smallest at either end, largest in the middle. It's often nice to see a uniform set, but also nice to have a mix which go together, but are perhaps not all exactly the same. Eventually after a year or two you'll find your beads end up similar sizes more easily.
You could try making a bead out of blue tack, and keeping it by you for reference.....I do this when I'm using my lentil press...it's hard to visualise how much glass you need to fill it.
Or make lots of beads and then match them up afterwards. I used to do this when I was throwing pots with lids....make lots of pots, lots of lids, and then some of them are bound to fit, and keep the odd ones for next time!
I made a sample bead the size I wanted on an undipped mandrel so it was permanently on there and annealed it. Then I used it as a visual guide for the set by holding each subsequent bead next to the the sample one and checking for size.
The difficulty is of course that cold glass is smaller than hot glass!
Quote from: Kaz on November 06, 2010, 10:50:01 PM
The difficulty is of course that cold glass is smaller than hot glass!
Just what I was going to say!
agreed, but the set in the kiln still turn out the same size as each other. Maybe should have pointed out they'll be slightly smaller than the sample bead :-[
It's a good idea Helen ;D
Just echoing what the others said really...it's a combination of good ideas like reference beads and marking mandrels, plus PPP. Several years down the line I'll still struggle to make a set of exactly the same size beads if I shape by hand, - but then I don't make beads every day so I guess if I practice more I'll get there ;D
Quote from: Kaz on November 06, 2010, 10:50:01 PM
The difficulty is of course that cold glass is smaller than hot glass!
this is true but to be fair the difference in size for 104 glass is something like 0.0000104mm (or percent - can't remember which) per 1cm3 for every 1 degree C rise in temp so its not exactly massive... but PPP ;D
Are you sure Anna - because when I pull murrini there is a massive difference between the pull diameter when it's hot and when it has cooled thoroughly?
Or is it that glowing glass appears bigger?
Kazx
[/quote]
this is true but to be fair the difference in size for 104 glass is something like 0.0000104mm (or percent - can't remember which) per 1cm3 for every 1 degree C rise in temp so its not exactly massive... but PPP ;D
[/quote]
But the eye just could not detect this level of difference and I too notice the difference when making several spacers on one mandrel.
But maybe as Kaz says the glow gives the appearances of a molten glass being bigger than cool glass?
I have a pair of metal calipers and slip the hot bead through the gap to check. This makes things super accurate. I used to do it by eye, which was also pretty good - I can tell you how big 13mm or 16mm is just by looking now. I suppose that does come with practise.
I happen to think that unless a customer particularly demands it it's nice to have a little variation in size. We're making handmade things for goodness sakes - we may as well be machines if we spend all day using presses and shapers.
Okay - I'll concede that people who like their Pandora style beads want them all the same size but most other people are happy to have a nicely matched but size graduated set of beads.
I just wrote a big reply to this and now its gone.... has anyone seen it? Ok it went along the lines of:
hot glass is less viscous than cool glass thus has entirely different properties due to the very nature of glass as a material. The fact that glowing glass is simply so hot will also effect the air in the immediate vicinity of the bead and thus distort the image we have of it (all fuzzy, blobby and rounded generally). The teeny tiny figure I quoted needs to be multiplied by between 800-1100 as that is at what temp we heat our glass to to make it do its thing - this is still very tiny but significantly different to looking at the figure of COE as a simple formula against 1cm3 of glass at 1degree C.
Def way too technical for a sunday morning. I'm off to go melt some glass now!
I tried putting a dot with permanent marker on some of my mandrels, below where the bead release would be, so that I could tell how many wraps I'd done without losing where the start point was. It didn't help a huge amount because my individual wraps aren't that similar in size!
If you're making simple beads you can try doing a pair to a mandrel, so you can compare them to each other. But yeah, mainly just practice - I can make a number that are fairly close in size now.
Also, if you've got a doming block, that can help if you compare them against the same dip, maybe roll them gently in it.
i use my doming block, make a bead the size of a hole, then if it needs to be bigger i count the number of wraps i add, being as its only usually a few, but after the first few i can eyeball the size easily! It is just the old hat of PPP and then one day you'll just find it clicks!
funny enough, my core beads usually turn out the same size as each other, unless I fluff something and then do a salvage operation! I wouldn't be very receptive to a customer wanting a set where they are all identical, for me it would take the point (and the fun) out of handmaking my own beads. Having said that some of the beads I really admire and drool over are very precisely made :)
Oh, the other thing I do, if the beads are relatively simple, is to make them on the same mandrel. It's always a challenge to keep everything hot. Works great for simple spacers and earring pairs though.
I sometimes make 2 spacers on one mandrel (when I'm feeling brave), and the second one always looks a bit bigger than the first until it has cooled a bit.
Apart from beadrollers I found an ancient pair of calipers in the garage and I find it a great help.