Title: How to work Effetre Red Roof Tile
Post by: Sarah9959 on November 05, 2010, 04:44:20 PM
Should have asked when I bought it I guess, but didn't.

How should I work this on HH to get a nice rich colour - first attempts just reveal dull browny beige.

Thanks     Sarah
Title: Re: How to work Effetre Red Roof Tile
Post by: Kalorlo on November 05, 2010, 06:35:47 PM
The stuff I have can strike darker if you work it for a while - heat, cool, in, out, etc. I have a photo somewhere from a while back:

(http://farm2.static.flickr.com/1414/4601955877_76c2b87bf7_m.jpg) (http://www.flickr.com/photos/kalorlo/4601955877/)

Just with SIS. I think the spacer on the left was giving me difficulties so I took a long time shaping it.