Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Kilns => Topic started by: Tills on November 02, 2010, 01:58:28 PM

Title: SC2 Kiln question
Post by: Tills on November 02, 2010, 01:58:28 PM
Hello all, I wonder if anyone can remind me of how I can increase my 'garaging' (Hold Time) mid session... since we moved some of our things are in storage and my instruction book amongst other things is in there.

Any help is appreciated, -finished for today, could have done with an extra half hour, but would be useful for future sessions.

Thanks

Title: Re: SC2 Kiln question
Post by: Trudi on November 02, 2010, 02:10:46 PM
Not sure if there is a better way - but you could start off the programme again - as you run through the stages you can increase the time!

I tend to have mine set to garage for about 12 hours and I skip the segment when I'm done! HTH!
Title: Re: SC2 Kiln question
Post by: mariag on November 02, 2010, 02:14:06 PM
Hi Gail, you can download instruction manuals from Paragon
http://www.paragonweb.com/Instruction_Manuals.cfm
Title: Re: SC2 Kiln question
Post by: Tills on November 02, 2010, 02:23:47 PM
Brill, thank you both! Much appreciated! Gail x