Post by: jammie on October 23, 2010, 10:08:19 AM
well I have searched here and looked in my books but cant find the answer. I would really like to have a go at one but cant work out how to do it.  ???
Title: Re: how do you make a spine bead
Post by: Redhotsal on October 23, 2010, 10:21:11 AM
Very quickly:
Make a core barrel in a darkish colour - shape like a very long lemon. Marver until smooth.
Take a clear rod and add a thick spiral of clear from one end to the other. Don't let the coils touch each other. Alternately - add sepearate rings of clear around the core.
Melt in slowly. Don't marver or reshape - you want the clear to sink straight down into the core.
When smooth encase properly with clear.
Squash gently to emphasise the "spines".
Job done  :)
Title: Re: how do you make a spine bead
Post by: Lush! on October 23, 2010, 10:25:50 AM
Bish Bash Bosh  ;D ;D
Title: Re: how do you make a spine bead
Post by: fionaess on October 23, 2010, 12:10:51 PM
Its also known as a tornedo bead :) 
Title: Re: how do you make a spine bead
Post by: kathsd on October 23, 2010, 04:58:09 PM
thanks for the nice simple instructions, I was thinking about giving one of these a go,  and now I know how (rather than guessing! ) I'll head back to the torch and give it a shot.
Kath
Title: Re: how do you make a spine bead
Post by: Kaz on October 23, 2010, 05:21:54 PM
And for serious gorgeousness make the base colour a silver glass one!
Kazx
Title: Re: how do you make a spine bead
Post by: Blue Box Studio on October 23, 2010, 07:18:27 PM
Anyone have a pic of what these look like?  Not heard of them before and being a newbie I like to know what the end result is supposed to look like before I tackle something new. 

Shame I don't apply the same criuteria to my cooking - DH eats some strange things  and sometimes asks 'is it meant to look like this?'.
Title: Re: how do you make a spine bead
Post by: Princess Peggy (Priscilla McGirr) on October 23, 2010, 08:10:37 PM
Thank you Sal.....I've been puzzling about how to do these for a while, now I can have a go.   Pris
Title: Re: how do you make a spine bead
Post by: Teddie on October 23, 2010, 08:18:22 PM
There is a lovely picture of one of these beads on page 3 of this weeks gallery. :)
Title: Re: how do you make a spine bead
Post by: Dragonfire Glass on October 23, 2010, 09:03:15 PM
my avatar is a tornado bead  ;D
Title: Re: how do you make a spine bead
Post by: beadysam on October 23, 2010, 10:26:30 PM
Archived page of the Margaret Zinser Tutorial - no piccy here, but I have it saved somewhere if you are desperate?

http://web.archive.org/web/20080526012925/http://www.mzglass.com/twistytutorial.htm
Title: Re: how do you make a spine bead
Post by: Blue Box Studio on October 23, 2010, 10:38:35 PM
Oh wow!  They are stunning.
Title: Re: how do you make a spine bead
Post by: Princess Peggy (Priscilla McGirr) on October 25, 2010, 06:15:13 PM
Well, I had a go and here it is!  Thanks Sal for unraveling the mystery!

(http://farm2.static.flickr.com/1054/5114977380_c1d0001431.jpg) (http://www.flickr.com/photos/50810791@N03/5114977380/)
spine bead with Aurae (http://www.flickr.com/photos/50810791@N03/5114977380/) by Princess Peggy1 (http://www.flickr.com/people/50810791@N03/), on Flickr
Title: Re: how do you make a spine bead
Post by: awrylemming on October 25, 2010, 06:17:54 PM
I made two lovely beads, but neither survived  :'( Perhaps because I used a frit base, still the next one will survive and now I know how - thanks everyone  ;D 
All the beads are lovely, I've always liked this particular style.
Title: Re: how do you make a spine bead
Post by: jammie on October 25, 2010, 11:03:15 PM
Thank Sal!  :)
Thats a lovely bead Peggy!
Mines were poop, but it was fun trying. My second one was better but cracked on the inside as i think it took so long to get the clear on.
Will try again though. It was fun making them. Thanks for the link too Sam.
It was your avatar pic that  set me wondering how they were made Fallariel  :D
Title: Re: how do you make a spine bead
Post by: Shirl on October 27, 2010, 06:26:56 PM
Thanks for the info.
What a stunning bead, I might have a try at one of these later.
Title: Re: how do you make a spine bead
Post by: ScarletLeonard on October 27, 2010, 08:11:07 PM
Oh oh oh.

Thanks Sal for the rundown I'm mid session atm  so know what I am doing when I finish the set I'm on.
Title: Re: how do you make a spine bead
Post by: Tracy on October 27, 2010, 08:26:38 PM
I love making tornados, not made any in ages, I use clear stringer to make the spirals
(http://i707.photobucket.com/albums/ww72/ace_balloonz/Dec%2009%20Sets/th_IMG_1429.jpg) (http://s707.photobucket.com/albums/ww72/ace_balloonz/Dec%2009%20Sets/?action=view&current=IMG_1429.jpg) (http://i707.photobucket.com/albums/ww72/ace_balloonz/Beads%2010/th_IMG_1897.jpg) (http://s707.photobucket.com/albums/ww72/ace_balloonz/Beads%2010/?action=view&current=IMG_1897.jpg) (http://i707.photobucket.com/albums/ww72/ace_balloonz/Beads%2009/th_IMG_1970.jpg) (http://s707.photobucket.com/albums/ww72/ace_balloonz/Beads%2009/?action=view&current=IMG_1970.jpg)
Title: Re: how do you make a spine bead
Post by: Redhotsal on October 28, 2010, 12:09:24 AM
Quote from: Princess Peggy on October 25, 2010, 06:15:13 PM
Well, I had a go and here it is!  Thanks Sal for unraveling the mystery!

(http://farm2.static.flickr.com/1054/5114977380_c1d0001431.jpg) (http://www.flickr.com/photos/50810791@N03/5114977380/)
spine bead with Aurae (http://www.flickr.com/photos/50810791@N03/5114977380/) by Princess Peggy1 (http://www.flickr.com/people/50810791@N03/), on Flickr

Wow, Pris, that's gorgeous!!  :P (drool)
Title: Re: how do you make a spine bead
Post by: GoldenGlassGirl on October 28, 2010, 12:17:28 AM
Lovely bead but how do you keep the silvered glass colours? I have been practising with non silvered glass and have cracked the technique (well - nearly!) but when I tried with a rod of DH Elektra all the colours disappeared. Did I chose a bad glass to try this with or was I melting down too quickly? ???

Sandra