Title: Can you get coe 90 tubing?
Post by: elburnzo on October 20, 2010, 12:33:20 PM
well the title says it all. is this in existence? and if so where can you get it?
Title: Re: Can you get coe 90 tubing?
Post by: Flyingcheesetoastie on October 20, 2010, 12:34:32 PM
Does Schott do a 90COE?
Title: Re: Can you get coe 90 tubing?
Post by: elburnzo on October 20, 2010, 12:41:55 PM
had a look on their website- completely confused lol. i guess a 104 tubing would maybe work, but might be too soft. wanted to try some xmas decorations but dont have the fire power for boro.
Title: Re: Can you get coe 90 tubing?
Post by: garishglobes on October 20, 2010, 12:45:02 PM
Did Sean at Off Mandrel have some at one point?

If you're feeling really brave, you could try what I saw Di East doing, and make your own tubing on the end of a blowpipe - or actually, curl clear on the end of a blowpipe and blow as if making shards, just make the ball thicker.
Title: Re: Can you get coe 90 tubing?
Post by: SilverGems89 on October 20, 2010, 01:03:31 PM
yes Sean has Schott 10mm tubing
Title: Re: Can you get coe 90 tubing?
Post by: elburnzo on October 20, 2010, 01:43:52 PM
Quote from: SilverGems89 on October 20, 2010, 01:03:31 PM
yes Sean has Schott 10mm tubing

duh dont know how i managed to miss tht when i was looking earlier! thanks guys xxx
Title: Re: Can you get coe 90 tubing?
Post by: Ian Pearson on October 20, 2010, 01:45:14 PM
I have some 90. Think its Schott AR. Some spare for free if anyone wishes to email me