I came across a make of glass called "Beadmaking 104 glass" online here: http://artistryinglass.on.ca/store/catalog/BEADMAKING_104_GLASS_page_1_c_379.html

I am not intending to order, but was rather intrigued by it as I've never heard of it before.  Has anyone used it?  Some of the colours seem rather expensive - is it some kind of miracle glass?  :o
Title: Re: Beadmaking 104 Glass?
Post by: mizgeorge on October 16, 2010, 10:09:04 PM
I think these are Kugler aren't they?
Title: Re: Beadmaking 104 Glass?
Post by: Hazer on October 16, 2010, 10:14:04 PM
Yeah, pretty sure it's Kugler; there's a rod called Bahia Blue there, which fits.
Title: Re: Beadmaking 104 Glass?
Post by: Kaz on October 16, 2010, 10:16:51 PM
Emma still has some of this for sale and a lot cheaper.
http://www.garishglobes.co.uk/section.php/69/1/glass-for-beadmaking
Kazx
Title: Re: Beadmaking 104 Glass?
Post by: helbels on October 16, 2010, 10:29:42 PM
Is it nice?  :D
Title: Re: Beadmaking 104 Glass?
Post by: Kaz on October 16, 2010, 10:54:03 PM
Oh yes it's lovely but sometimes some compatibility issues with standard 104. Great base for silver glass thought especially those neutral/brown colours.
Kazx
Title: Re: Beadmaking 104 Glass?
Post by: Sarah on October 16, 2010, 11:05:20 PM
If I remember rightly its the ASK range which Arrow Springs (AS) ditched because of the compatibility and consistency issues but Kugker (K) continued. Beautiful glass if a bit frustrating at times.

Sarah
xxx
Title: Re: Beadmaking 104 Glass?
Post by: Kaz on October 16, 2010, 11:26:23 PM
Still had one or two compatibility issues for me but I love this glass.