Text only
|
Text with Images
Frit-Happens !
Lampwork => Lampworking Tip n Tricks => Topic started by: Trudi on October 08, 2010, 05:50:08 AM
Title:
Shocky glass tips
Post by:
Trudi
on
October 08, 2010, 05:50:08 AM
I found this frantz blog that has some good tips
http://frantznewsletter.com/?p=2322#comments
Title:
Re: Shocky glass tips
Post by:
jammie
on
October 08, 2010, 09:12:23 AM
Has anyone tried putting them in the kiln like this? Is it worth doing if you have? :)
Title:
Re: Shocky glass tips
Post by:
liquidglass
on
October 08, 2010, 11:42:12 AM
Very interesting, thanks Trudi.
Text only
|