Frit-Happens !

Lampwork => Borosilicate => Topic started by: hollergrafik on October 05, 2010, 04:52:31 PM

Title: Boro hates me ......
Post by: hollergrafik on October 05, 2010, 04:52:31 PM
... and to be honest I hate it too  :(

I recently bought some to give it a go, I am on 2 oxys and a mini CC but I lose the will to live trying to melt the stuff, I will bung it up in swaps and go back to my 104 <3
Title: Re: Boro hates me ......
Post by: garishglobes on October 05, 2010, 04:56:03 PM
If you're on 2 oxys and a mini cc, you shouldn't be losing any will to live melting boro. It is slower and thicker and handles differently to clear glass but it shouldn't be impossible, and certainly not with that firepower.
As a boro fanatic, I'd love to help if I can.... what are you trying to do with it? Do you have problems melting clear boro on its own?
Title: Re: Boro hates me ......
Post by: hollergrafik on October 05, 2010, 05:01:12 PM
I bought Caramello light, went nice murky green and sable something (followed your reducing instructions) had the most miniscule amount of whispy blue. The clear I have is Simax ??

it takes me an age to even get it flowing enough to wind on the mandrel, probably 3 mins of constant heat and then thats only enough for one wrap.
Title: Re: Boro hates me ......
Post by: awrylemming on October 05, 2010, 07:52:54 PM
Don't give up!!  Remember what it was like learning to use 104, all the frustration then the hurrah moments.  Give it a go (and sell em to me afterwards, yum  ;D)

Sue x
Title: Re: Boro hates me ......
Post by: ♥♥Tan♥♥ on October 05, 2010, 07:55:39 PM
Something isn't right there, you certainly have the firepower to melt it, daft question, are the rods a reasonable thickness?
Title: Re: Boro hates me ......
Post by: hollergrafik on October 05, 2010, 08:13:17 PM
Emma Kindly went through some pointers with me, gonna pull the rods into fat stringers. I was trying to melt fat rods.
Title: Re: Boro hates me ......
Post by: garishglobes on October 05, 2010, 08:15:10 PM
I think....the rods may be too thick. It does sound as if there is plenty of firepower, but boro is a different animal and requires a different mindset to work it. I've pm'ed you anyway, but just to say here - I'd suggest pulling 2-3mm stringer (remember you often only need small amounts of colour because boro colours can be a lot more saturated than the soft glass ones), wrapping that round the mandrel and then encasing with a 4mm rod of clear.
You can make lovely fritty beads with a wrap of a colour then a couple of rolls in frit, then 2 or 3 wraps of clear and melting it all in.

Clear is definitely "runnier" than other boro colours too (followed by amber purples, some greens and then the blues, some of which are really stiff) so using more clear makes the bead easier to shape.

ETA: beat me to it!!  ;D
Title: Re: Boro hates me ......
Post by: Hotglass28 on October 17, 2010, 05:42:32 PM

Kay, you NEED to be good at Boro...... You needs to be  ;)

One day I'd like to give it a go. I like the idea of going slow and being able to make bigger stuff one day.

For now, 104 has me hooked and shall stay that way. But I'd love to see you make stuff in Boro.

Denise
Title: Re: Boro hates me ......
Post by: hollergrafik on October 17, 2010, 06:40:55 PM
Given up on it LOL
Title: Re: Boro hates me ......
Post by: ♥♥Tan♥♥ on October 17, 2010, 06:56:25 PM
I am just about to start on this boro journey, I hope I have better luck :-\
Title: Re: Boro hates me ......
Post by: hollergrafik on October 17, 2010, 06:58:37 PM
I just dont have the patience Tan, cant be naffed with it taking ages and only being able to do boro on its own and not make 104 beads at the same time as the kiln temps are very different
Title: Re: Boro hates me ......
Post by: ♥♥Tan♥♥ on October 17, 2010, 06:59:47 PM
That is my initial concern........I guess it will be a steep learning curve, I have some clear some shorts and some frit and I'm aiming to keep it simple in the beginning and see how I feel about it rather than rush at it and buy loads of glass then discover I hate it
Title: Re: Boro hates me ......
Post by: hollergrafik on October 17, 2010, 07:05:39 PM
Quote from: Tan on October 17, 2010, 06:59:47 PM
see how I feel about it rather than rush at it and buy loads of glass then discover I hate it

Yeah I know that one, coming to a for sale section soon LOL
Title: Re: Boro hates me ......
Post by: ♥♥Tan♥♥ on October 17, 2010, 07:13:45 PM
Well, looking at the other side of it, imagine if you had loved it then you would have had all that lovely glass to play with
Title: Re: Boro hates me ......
Post by: hollergrafik on October 17, 2010, 07:32:00 PM
It was worth a go, I had to get some other stuff to see if it was maybe the colours I didnt like, hey ho  ::)
Title: Re: Boro hates me ......
Post by: Hotglass28 on October 17, 2010, 09:32:21 PM

Like someone said, it's a different animal. I guess you have to re learn all over again for Boro.

I like the idea that you it can stay out of the flame for a bit longer while you work it.

Silver clay hates me, that's my hate, I haven't said a bad word to it but the stuff just is evil to me  ;D

Tans got a good point, if you did like it I think your bank balance would take a hit, its not cheap stuff is it  ;) 

Denise
Title: Re: Boro hates me ......
Post by: Steampunkglass on October 17, 2010, 11:03:25 PM
Quote from: Hollergrafik or Special Kay :) on October 17, 2010, 06:58:37 PM
I just dont have the patience Tan, cant be naffed with it taking ages and only being able to do boro on its own and not make 104 beads at the same time as the kiln temps are very different
If you want to work both glasses at the same time you can always chuck it in the kiln at the normal 104 schedule, then do a batch anneal later for all the boro at the higher temperature. The only problem you'd have with that is the risk of mixing up the glasses.

I did the same as Tan, tried some clear to get used to melting it, then added a very few colours. Use lots of clear, it's cheaper and melts easier. I think of the colours like concentrated paint, and you use the clear to thin it down, layering it ontop or underneath to make it go further  ;)