Hi all,
I tried this for the first time tonight (just a quick test bead) and it was bubbling and boiling like a good un - is it just me? Or has anyone else found this?
Helen x
it can bubble a little - I just nip the ends off and when I go to heat the glass leave the very edge of it just outside the flame - that should help!
I agree with Trudi - only the end bubbled initially
Thanks ladies, won't panic just yet then ;D
http://dragonjools.blogspot.com/2010/09/cim742-2-sepia-blue-variant.html (http://dragonjools.blogspot.com/2010/09/cim742-2-sepia-blue-variant.html)
Not just you! Pretty colour, though 8)
Mine went like a volcano :o when melting but I loved what came out of my kiln the next day. I have fallen in love with this colour so much , that the first bracelet I made I decided to keep as I loved the finish that much. Plus I have had 2 orders for more of that same colour . :o :o
So I have bought sepia to try as well I hope I like the results in that colour