It's probably something really simple, but I would appreciate some help guys!!
I absolutely love the "stony organic" effect that comes with silvering ivory and I bought myself a book of silver foil sheets, so that I could have a go at achieving this myself. However, I'm not getting the results that I hoped for!
I have had two attemps now - here's what I've done. I've made a plain ivory bead, rolled it in the silver and then burnished it off. The first time I did this, the effect was very "metallic" than stony. Les very kindly gave me a tip and told me to really chuck a lot of heat at my next bead - the first one I burnished very gently at the top of the flame, so I made one yesterday and really heated it well.
But the effect was still the same. ???
What am I doing wrong? Should I be making an ivory bead and then adding some silver ivory stringer into it, rather than rolling it directly into the silver foil? Am I using too much silver? Am I not heating it for long enough??
Would really appreciate some guidance! Unfortunately no pic to put up until tomorrow, sorry.
Thanks very much!
x
Hi Rachel,
Do you have any pics of what you've got so far and any examples of what you're after? You don't need an awful lot of silver to get some reactions and foil is quite thick...maybe less foil is required for the look you're after.
Hazel xx
What you need to do is just take a thin strip, much less than the width of your bead, roll the bead over it and then take it out of the flame and burnish it on with a nearby handy tool, work quickly though. Then back into the flame and heat heat heat, you will be able to see the reaction happening so you will know its right
Quote from: Sulis on September 12, 2010, 12:56:06 PM
Hi Rachel,
Do you have any pics of what you've got so far and any examples of what you're after? You don't need an awful lot of silver to get some reactions and foil is quite thick...maybe less foil is required for the look you're after.
Hazel xx
Hi Hazel,
Thanks for this. The effect that I'm getting is evidenced in the photo that I put up in the Gallery under First Beads - the one that is entitled "What came out of the annealing bubbles this morning." It is the first bead on the left, with the stripe of dark amber across it.
The affect that I want to achieve is sort of the old "stony" look, mottled like marble if this makes any sense??? ;D
Quote from: Tan on September 12, 2010, 12:58:27 PM
What you need to do is just take a thin strip, much less than the width of your bead, roll the bead over it and then take it out of the flame and burnish it on with a nearby handy tool, work quickly though. Then back into the flame and heat heat heat, you will be able to see the reaction happening so you will know its right
aha!! Thanks Tan! That is really helpful - I shall have another bash this afternoon!
When you say burnish it on, do you mean roll it on my marver say, to spread the silver around, after it has been melted in? Then put it back in the flame and really throw some heat at it??
Hi Rachel, Burnishing means to use a metal tool and rub it over the silver once it's attached to your bead. Basically it makes sure your silver leaf is stuck on good and proper. As the silver is very fine if it's not attached properly it will just burn away in the flame.
Hi Rachel,
Ok, I know what you mean :) I think Tan and Stacy have the best advice there. When I burnish, I make sure that the bead is cool enough so you can tap it gently with your paddle and it's hard before I start to rub the silver in. I don't know if that will also help.
Hazel xx
I prefer to make silvered ivory stringers. I use leaf rather than foil and make sure that I apply them to the base without covering all the surface. Then I heat them like mad, let the bead droop about all over the place and reshape. I love watching the actual reactions happening :)
silvered stringer works well, its quite easy to use, well I find it easier than rolling in the silver, but I have leaf not foil. There's a couple of tutorials on here about them, I can find them if you would like them. :)
Quote from: jammie on September 12, 2010, 03:31:13 PM
silvered stringer works well, its quite easy to use, well I find it easier than rolling in the silver, but I have leaf not foil. There's a couple of tutorials on here about them, I can find them if you would like them. :)
If you don't mind Jammie that would be great, thank you! ;D
http://www.frit-happens.co.uk/forum/index.php?topic=9716.0
http://www.cauldroncreations.com/sistutorial.html
http://www.frit-happens.co.uk/forum/index.php?topic=9638.15
http://www.frit-happens.co.uk/forum/index.php?topic=2160.0
there you go ...my favourites, should keep you going for a while! ;D
Thankyou!! ;D
Yaaaaaaay!! Success!!! ;D ;D ;D ;D ;D
Great >: ;D
make sure you show us your results :P