Frit-Happens !

Lampwork => COE 104 => Topic started by: Fruddy on September 02, 2010, 12:47:18 PM

Title: Shards - How do you Use 'Em??
Post by: Fruddy on September 02, 2010, 12:47:18 PM
You just know that I'm going to be a total glass addict, in every sense of the word!  Not even set up yet and am collecting glass, frit, murrini and shards at an alarming rate of knots!!! :)

I'm pretty okay with how to use frit and murrini, but what about shards??    How best to apply them?

Any advice gratefully received!

Thanks v. much. ;D
Title: Re: Shards - How do you Use 'Em??
Post by: garishglobes on September 02, 2010, 01:08:18 PM
There's a short explanation here -

http://www.frit-happens.co.uk/wiki/Shards (http://www.frit-happens.co.uk/wiki/Shards)

Title: Re: Shards - How do you Use 'Em??
Post by: Fruddy on September 02, 2010, 01:58:26 PM
Thank you, that's really helpful!

My brain hurts from trying to cram all this new knowledge into it!!! ;D
Title: Re: Shards - How do you Use 'Em??
Post by: Jolene on September 02, 2010, 03:20:18 PM
Just added a link on the wiki to my video tutorial that I put on YouTube a while ago. ;D
Title: Re: Shards - How do you Use 'Em??
Post by: Fruddy on September 02, 2010, 04:59:20 PM
Excellent, thanks Jolene. :D