Frit-Happens !

Lampwork => Common Problems => Topic started by: shaz on August 30, 2010, 02:35:31 PM

Title: Another question NYX ?
Post by: shaz on August 30, 2010, 02:35:31 PM
Sorry me again ;D, just used a thin rod and all it has on the label is NYX ? I tried it on some ivory and its gone metallic anyone know what it is?
thanks Sharon
Title: Re: Another question NYX ?
Post by: Jolene on August 30, 2010, 02:37:26 PM
It is a double helix reduction glass... http://www.doublehelixglassworks.com/nyx14lb.aspx ;D Yum!
Title: Re: Another question NYX ?
Post by: shaz on August 30, 2010, 02:43:45 PM
Thanks just looked at that site :o is this going to be an expensive pastime? ;D  Its just metallic at the moment so dont suppose I will get the full effect till I get a kiln then will I?  roll on crimbo (not holding my breath)
Title: Re: Another question NYX ?
Post by: AnnaSpanna on August 30, 2010, 02:58:02 PM
Shaz,

there are lots of different silver glasses fromm DH amongst others. Some will remain as metallic or swirly as they are even if they go in the kiln. Some will lose their metallicness in the kiln (always depressing) if they don't go straight in from the torch. Some will not even bloom in colour until they get to the kiln! Yes silver glass can be an expensive but beautiful aspect of lamping. As you plough on through your glassy discoveries you will find various other "cheaper" glasses that have metallic and other amazing reactions so don't worry about the DH for the mo! We all go through the "silver glass" phase and some of us have yet to come out of the other side!

Enjoy and don't look at the price tag!
Title: Re: Another question NYX ?
Post by: shaz on August 30, 2010, 03:35:16 PM
Didnt know it was best for them to go straight to kiln, so should I save the rest till I get my kiln?
Title: Re: Another question NYX ?
Post by: helbels on August 30, 2010, 03:48:37 PM
Nyx is a kiln striking glass so I would wait until you have a kiln to use the rest of it, otherwise you won't be getting the full effects.
Title: Re: Another question NYX ?
Post by: jammie on August 30, 2010, 07:37:03 PM
I tended to leave the more expensive or maybe difficult glass until I could do not too bad with the cheaper glass. Practicing with plain glass always felt better because wasting it didn't hurt so much!  :)