Frit-Happens !

Lampwork => Lampworking Tip n Tricks => Topic started by: lampworklover on August 20, 2010, 10:24:48 PM

Title: ..my next question...
Post by: lampworklover on August 20, 2010, 10:24:48 PM
okay, I guess that as we progress though our lampworking careers we will all get asked these sorts of questions....and I'm pleased to say that this one doesn't involve hair of any sort!!

Customer has contacted me and asked me if I can add a name to a bead  ???.. I thought maybe alphabet murrini (although I don't make murrini yet), or possibly engraving the name on a tab bead with my electric bead reamer. I'm wracking my brains to come up with a suggestion that doesn't look naff to be honest!

any ideas please peeps?
Title: Re: ..my next question...
Post by: elburnzo on August 20, 2010, 10:28:39 PM
paint it with rachel elliots enamel paints?
Title: Re: ..my next question...
Post by: Black Heart Beads on August 20, 2010, 10:33:37 PM
You could write with fine stringer (but this would be beyond me) or coat a bead in enamel and then engrave with your reamer, reheat and fire polish to get a nice finish.
Title: Re: ..my next question...
Post by: Hazer on August 20, 2010, 10:35:38 PM
Ooh, that's a good idea - I'd been thinking about Becky's transfers, but she doesn't sell individual letters (which made me wonder if you could cannibalize some of her existing words ones to spell out the name :D)
Title: Re: ..my next question...
Post by: garishglobes on August 20, 2010, 10:41:00 PM
Becky can do custom transfers from a jpeg image  :)
Title: Re: ..my next question...
Post by: LittleHen on August 20, 2010, 10:55:40 PM
Zoozis do name plate press systems but quite pricey if you just want to make 1 bead 1 time.
I think it'll be interesting to see what you come up with.
Have you thought of pmc or stamped silver tags next to lovely lampwork?
Title: Re: ..my next question...
Post by: beadysam on August 20, 2010, 11:04:18 PM
What about etching with a resist?  Subtle effect but do-able!
Title: Re: ..my next question...
Post by: Veebee on August 20, 2010, 11:16:19 PM
Quote from: beadysam on August 20, 2010, 11:04:18 PM
What about etching with a resist?  Subtle effect but do-able!

If you already have etchig solution this would be a really cost effective way of doing what you want to do.
Title: Re: ..my next question...
Post by: lampworklover on August 20, 2010, 11:34:22 PM
Now that idea I like; I tried using PVA glue as a resist the other week and it worked a treat, plus I have a very fine nozzled bottle of glue.

Thanks all of you!!
Title: Re: ..my next question...
Post by: Pat from Canvey on August 21, 2010, 07:09:01 AM
This was an experiment I did last week
(http://pic20.picturetrail.com/VOL1426/5604171/22750186/390702756.jpg) Tracing black and clove oil and a fine nibbed pen on a cold bead and then re-fired in the torch after pre-heating in the kiln. Just have the get the consistency of the "ink" right for a better outcome.
Title: Re: ..my next question...
Post by: Sonja on August 21, 2010, 10:06:43 PM
If you want to try some letter murrini... I have it in dark blue with a white letter in the center.
What letters do you need and I can make a picture.
:)