Title: can you use an oxyacetylene gas welding torch for lampwork?
Post by: the lady with the lamp on August 17, 2010, 10:42:43 AM
 ??? Me and my partner are setting up a home workshop up together,hes into classic cars and metalwork he wants to know if we can use an oxyacetylene torch as used in gas welding for lampwork?
Title: Re: can you use an oxyacetylene gas welding torch for lampwork?
Post by: Ian Pearson on August 17, 2010, 10:54:43 AM
You can use the torch but better to use propane rather than Acetylene. Depends on type of work you want to do as "lampwrok covers a wide range. I have in past use hand torches designed for welding and brazing but always with propane.

Ian
Title: Re: can you use an oxyacetylene gas welding torch for lampwork?
Post by: flaming beads on August 17, 2010, 10:57:30 AM
Not really a lot of help on this, but think the propane gives the right heat needed for the glass!?!?...someone with better knowledge will come along though...good luck in your set up...it sounds like fun!! ;)
Title: Re: can you use an oxyacetylene gas welding torch for lampwork?
Post by: paintboxcrafts on August 17, 2010, 11:34:44 AM
I think an Oxy-acetylene flame is not clean enough, you would get black smuts.
It is also a lot hotter, 3500C as opposed to 2500C, according to wikipedia.
Cathy
Title: Re: can you use an oxyacetylene gas welding torch for lampwork?
Post by: the lady with the lamp on August 17, 2010, 11:57:46 AM
thanks for input,forgot to say we will be using propane
Title: Re: can you use an oxyacetylene gas welding torch for lampwork?
Post by: ♥♥Tan♥♥ on August 17, 2010, 12:19:31 PM
I started out on exactly this set up, acetylene is a dirty gas and when its not depositing muck on the glass its boiling the heck out of it, I learned the hard way on that one ::) You will be fine with propane.

I had a Saphyre torch, still have it here somewhere, the one with exchangeable heads, it served its purpose but the flame wasn't really wide enough to do big beads, its a great little starter torch though and kept me going for years