Frit-Happens !

Lampwork => COE 104 => Topic started by: helenfc on August 09, 2010, 11:08:05 AM

Title: Recommend me some precision 104...
Post by: helenfc on August 09, 2010, 11:08:05 AM
A few of us are putting in a frantz order and they have precision 104  ;D ;D ;D
so I know sashas silver is meant to be a bit fab, is there anything else you guys would recommend? They had stopped selling it in the UK by the time I got my set up so any hints/tips would be much appreciated  :-*
Title: Re: Recommend me some precision 104...
Post by: Trudi on August 09, 2010, 11:24:47 AM
Hi

Rembrandt is very nice - green like Gaia but much easier to work with - it's a reducer!
Title: Re: Recommend me some precision 104...
Post by: helenfc on August 09, 2010, 11:26:44 AM
cheers trudi  :) any pics?  ;D
Title: Re: Recommend me some precision 104...
Post by: Kaz on August 09, 2010, 12:37:15 PM
Sacha's silver.
Would have said black pearl but see that it's out of stock - shame!
IMHO none of the precision 104 range is as good as DH. Probably why Martin stopped stocking it - so don't disappoint yourself by ordering tons of the stuff!
Kazx
Title: Re: Recommend me some precision 104...
Post by: Trudi on August 09, 2010, 12:56:24 PM


This was made using shards - looks much better IRL
(http://farm5.static.flickr.com/4097/4827529915_b510135101.jpg) (http://farm5.static.flickr.com/4097/4827529915_b510135101.jpg)

Where Gaia can be difficult - this one is very easy!

And I guess it's fair to say that many of the other preision colours were difficult to work - but this is good ans so is Sacha's. I think Katherin likes Black Pearl, I have some but haven't really had a good play with it to be fair!
Title: Re: Recommend me some precision 104...
Post by: dinah46 on August 09, 2010, 01:05:16 PM
Haven't had much success with precision 104 but loved sasha's silver when I first got it. Unfortunately the second lot was nowhere near as good for getting the colours.