Frit-Happens !

Technical Forum => Studio/workspace/setup/equipment => Tools and Presses => Topic started by: catriona on August 04, 2010, 01:20:38 AM

Title: fiber blanket
Post by: catriona on August 04, 2010, 01:20:38 AM
hi is this the type of fiber blanket i need for cooling my beads i use vermiculite at the momment but thought i,d give a fiber blanket a try also wheres the cheapest place to get them .

http://cgi.ebay.co.uk/1m-1-25mm-CERAMIC-FIBRE-BLANKET-KILN-FURNACE-/230493642988?cmd=ViewItem&pt=UK_Crafts_Ceramic_PotteryMaking_SM&hash=item35aa7de0ec


thanks xxcatxx
Title: Re: fiber blanket
Post by: Trudi on August 04, 2010, 08:17:13 AM
You'll get one from Martin or Sean for about £5 - I never really liked vermiculite!
Title: Re: fiber blanket
Post by: catriona on August 04, 2010, 08:50:20 AM
thanks trudie everyone i spoke ta lately says there much better.
off to order one now
xxcatxx
Title: Re: fiber blanket
Post by: Nikki on August 04, 2010, 10:10:34 AM
Cat I've got a fibre blanket I don't use, you can have it if you want. I prefer the annealing bubbles from Manda they are great.
Nikki
Title: Re: fiber blanket
Post by: beadysam on August 04, 2010, 01:43:56 PM
i've got body soluble ones at £4 if that helps.  The body soluble ones do what they say on the tin.  The fibres you inhale (and you will) will be absorbed safely by the body, rather than just sitting in your lungs causing untold problems long term....

http://www.beadysamglass.com/page38.htm   About half way down the page. ;)