When i finally get some torch time at the end of august i want to make some people/goddess type beads but I'm after a flesh coloured glass.
I know cim do ginger and butter pecan but wondered what you lot would reccommend as the all time best flesh coloured glass xxx
I was going to say butter pecan
i'm thinking this one too but i don't have any and before i order it just wanna see if there are alternatives.
saying that i did get a beautiful butter pecan unique from the states that is a cross between the colour of cream and butter pecan. yum! but a bit pale for skin :(
What about tongue pink? Will you be doing different flesh colours? There's some gorgeous chocolate browns too :)
maybe stoneground for oriental skin?
Quote from: Failariel on July 24, 2010, 09:59:55 AM
maybe stoneground for oriental skin?
oooo yeah, and i was thinking mink as well.
I think probably will have to try a few different bases, like ginger, butter pecan, and someone on LE suggested silver pink although tis quite expensive to use for a large bead. Saying that it's MUCH cheaper in the states so could always do a bulk/group order from frantz
CIM chai is a really nice fleshy colour, i made a goddess out of it and she looks lovely!
Effetre tongue pink with silver leaf is a gorgeous flesh tone :)
Quote from: helenfc on July 25, 2010, 11:50:53 AM
Effetre tongue pink with silver leaf is a gorgeous flesh tone :)
ooo got any pics? xxx ;D
Quote from: princess pink on July 24, 2010, 10:33:56 AM
Saying that it's MUCH cheaper in the states so could always do a bulk/group order from frantz
Be off with you, bad temptery person ;)
Kugler has a nice pink fleshcolour
Quote from: GlassOcean on July 25, 2010, 04:58:12 PM
Quote from: princess pink on July 24, 2010, 10:33:56 AM
Saying that it's MUCH cheaper in the states so could always do a bulk/group order from frantz
Be off with you, bad temptery person ;)
do you fancy it?? would have to be end of august when i'm back of hols...
Oh hello!!! ;D
i take it your in too them trudi?? right ok i will organize something the week i'm back off hols xx
I just used green for my witch beads ::) ::) ::) ::)