Frit-Happens !

Lampwork => Common Problems => Topic started by: ShinySnail on July 23, 2010, 10:12:33 AM

Title: My Mandrel Broke?
Post by: ShinySnail on July 23, 2010, 10:12:33 AM

Last night a bead I was making just fell to the desk, and when I looked I realised the mandrel had snapped.

Is this something that happens sometimes or have I done something that may have caused this?

???
Title: Re: My Mandrel Broke?
Post by: hollergrafik on July 23, 2010, 10:16:31 AM
sounds like you have over heated the mandrel and melted it, I did this on a couple of occasions when I was starting out.
Title: Re: My Mandrel Broke?
Post by: Dragonfire Glass on July 23, 2010, 10:19:59 AM
I think we have all melted througha manderel at some time!
Title: Re: My Mandrel Broke?
Post by: ShinySnail on July 23, 2010, 10:31:17 AM

Ahhhh thanks, yeah it was quite a big bead, and I had spent a while on it...

Didn't realise that I could do that - oops!

Thanks for the info
Title: Re: My Mandrel Broke?
Post by: flaming beads on July 23, 2010, 11:27:55 AM
Yup...i'm part of that club too :D....have kept it to remind me ;)