Have been away from the kiln for a couple of weeks and on my return found that the kiln has decided not to work. The working display after programming is showing a tCL message. Have looked it up in the book but doesn't really make it clear. Can anyone give advice please?
thanks xxx
Contact robin at cherry heaven (paragon kilns uk) - sorry I'm on my phone so can't give you a link right now.
Thanks, hubby working on it - brings back memories of electronics at uni apparently - rather him than me. Will keep Cherry Heaven in mind, not too far from me either!
x
http://www.cherryheaven.co.uk/kiln.htm
Have isolated the relay, have ordered from Cherry Heaven - should arrive tomorrow! Yeah!
thanks and fingers crossed.