Lampwork => Common Problems => Topic started by: Magpie on July 10, 2010, 09:56:02 PM

Title: I'm a big girl now....
Post by: Magpie on July 10, 2010, 09:56:02 PM
I picked up Vicky's oxycon last weekend and am all set up now on my big girl's torch (Carl's old Minor) and have enjoyed a couple of evenings playing. But Friday morning I noticed a 'leak'. When the torch is all off but the oxycon is running there is 'air' being blown out the side of the torch, close to where the oxygen hose attaches. When the torch is running it doesn't blow. Does the torch have a safety valve thingy that means if the oxy is on but not turned on at the torch it comes out of the valve so pressure doesn't build up, or do I have a leak that needs fixing?

Thanks
Title: Re: I'm a big girl now....
Post by: Kaz on July 10, 2010, 10:59:17 PM
Sounds like you have a leak to me if the oxygen is definitely switched off at the torch, Good idea to invest in some leak detector but as a last resort you can use soapy water to detect.
Kazx
Title: Re: I'm a big girl now....
Post by: julieHB on July 10, 2010, 11:23:45 PM
Deffo a leak. If you can hear it, and know where it comes from you don't need to "soap" it, but it should be fixed.

Don't keep the oxycon going for long with the torch closed - the oxycon does not like it!! I only turn the oxycon off at the torch for a few seconds while I light the torch, otherwise never. Even at the end of a session I never close the oxycon at the torch, only the propane after burning off all the gas in the propane hose.
Title: Re: I'm a big girl now....
Post by: beadysam on July 10, 2010, 11:27:55 PM
You should always have the oxygen open at least a litre or two whenever the oxycon is turned on - back pressure does an oxycon no favours.  Oxygen from the oxycon leaking isn't particularly dangerous but it should be a matter of routine to check all your connections regularly.  I use a spray bottle of water with a squirt of washing up liquid - its pretty much what is in the expensive commercial stuff.  Make sure you wipe off the connections with clean water, you don't want them to corrode in any way.

If you find your pipe isn't fitting well, take it off, cut off an inch and try again.  I soak it in hot water to make the pipe more flexible.  Hope that helps?  
Title: Re: I'm a big girl now....
Post by: Nick on July 10, 2010, 11:30:57 PM
Hi,

It could be that the hose connection is not quite secure enough. If not, it may be that the bit that the hose fits onto just needs a tighten with a spanner? Try putting some diluted washing up liquid around the joints to see if you get any bubbles. Hope this may help.

Regards
Title: Re: I'm a big girl now....
Post by: Magpie on July 11, 2010, 09:08:15 AM
Thanks all, I'll go play later after I've finished the computer stuff.