What is this?
Why have I nver heard of it ???
And most importantly, do I neeeed it?! :D
I have it, but what does it do? Or should it do something?
I don't think it "does" anything that spectacular, but from the photos I've seen it's a nice colour. Dragon Jools has tested it - you can read her findings here: http://dragonjools.blogspot.com/2009/09/effetre-441-dark-matter-follow-up.html and here: http://dragonjools.blogspot.com/2009/09/effetre-441-dark-matter.html
Julie Lush (secret tester!) has also tested it and written up here
http://www.tuffnellglass.com/contents/en-uk/d101.html
Kazx
I've put Aurae over it and got a nice metallic shine I have also tried reducing it heavily and get patches of a red copper lustre but can't get it over the whole bead - still playing ;D ;D
I haven't tried this...i'm feeling the need now though! ;)
Quote from: flaming beads on July 06, 2010, 07:55:56 AM
I haven't tried this...i'm feeling the need now though! ;)
really? ::) ;D
Ooohh..Julie...you're making me doubt myself now!!...i'm sure i haven't....there's still sooooo much i don't know! :o
Aah, right, not quite what I was expecting going by the colour of the paddle, but it does look interesting...probably worth a go! 8)