Can't remember what it's called but seen a silver glass that reduces to a shimmer turquoise. Possible by double helix. Any ideas?
Is it Gaia? :-\
Taxco silver, think its Tag?
Is it http://off-mandrel.com/index.php?main_page=product_info&cPath=65_70_76&products_id=362 ?
I have no idea, can u show me beadies with both?? Xx
Elektra 2 is a double helix Transparent glass....could it be this?
Sorry, I haven't tried the tag stuff - v. expensive, it just rang a bell when you said turquoise!
I have some elektra, I did wonder if you meant that - I have never really got on with it though.
ok stealing kate sullivans reef bead pic (which i am a proud owner of the bead) it's the tiny turquoise raised poked dots glass that i'm after!
(http://farm5.static.flickr.com/4014/4562481865_3abde26213.jpg)
looks like gaia to me ??? :)
I can get Black Nebula to go that shade if I heavily reduce it....
I get that from TAG Taxco
Hven';t used Gaia for a while...but do remeber sometimes getting it to do that!
Ask Kate!
Hi I used Tag Taxco over Cim Mermaid for the 3 larger beads and the small spacers were Cim Mermaid, just love this color.
Rita
http://www.flickr.com/photos/51048389@N02/4732917192/
Hi,
I vote for Electra 2. I have only used it once, but it fits the description you want.
Cathy
i'd vote for gaia, i've got a bead from kate that is a very similar colour and its gaia (and gorgeous of course!)
I vote Gaia too. I can get that colour by heavy reduction, burn it off a bit and flash in reducing flame.
Could be Abe's Ivy.
Is it this?
http://www.etsy.com/listing/46298998/taxco-silver-turquoise-single-rod (http://www.etsy.com/listing/46298998/taxco-silver-turquoise-single-rod)