Frit-Happens !

Lampwork => Common Problems => Topic started by: Liesly on June 16, 2010, 05:37:14 PM

Title: Annealing Bubbles
Post by: Liesly on June 16, 2010, 05:37:14 PM
This is a very green newbie question but................ Do I need to warm annealing bubbles or is the whole point that I can use them as they are?

How long should I wait before I put the bead into the bubbles - do I just plunge straight in?...... Not sure why I am so concerned I am sure my first attempts won't be worth keeping anyway!

I have just had some delivered and there are no instructions with them.

I also have a Bead Cube but I am too scared to turn it on  ::)

I have lurked for ages whilst gazing across at my hothead....

Liesl
Title: Re: Annealing Bubbles
Post by: Hazer on June 16, 2010, 05:41:58 PM
I'm a newbie too, but I use the annealing bubbles as is, in a large bowl, and it seems to work well - I haven't had any cracks due to the bubbles being at room temperature. Generally, I flash the bead in and out at the top of the flame when I've finished, wait a second, then put it into the bubbles. I've found that if I do it when the bead is too hot, I get pits where the bubbles embedded in the glass!

(I'm sure you already know this, but just in case, the annealing bubbles don't actually anneal the beads; they work like a fibre blanket or vermiculite, so getting your Bead Cube set up is the best option :) )

Good luck, and have fun :D
Title: Re: Annealing Bubbles
Post by: Liesly on June 16, 2010, 06:01:40 PM
Thanks for the advice

I think I may take the plunge this evening... I liked the idea of using the bubbles until I have  a few beads to anneal at once, I guess I will garage beads once I get going and have more confidence.

Thanks

Liesl
Title: Re: Annealing Bubbles
Post by: Kalorlo on June 16, 2010, 10:01:52 PM
Hold your bead in shade (possibly under the table) until you can see it's no longer glowing. Then put it in the bubbles and you know it won't get squished.
Title: Re: Annealing Bubbles
Post by: Jennie Lamb on June 17, 2010, 05:23:13 PM
Hiya Liesl......I use annealing bubbles too and agree with all that has been written thus far on their use! I also own a Bead Cube and tend to Batch anneal my beads and my advice would be :


:o DO NOT BE AFRAID  :o  

Your Bead Cube should be all pre-programmed for Garaging or/and Batch Annealing and it is SO easy all you have to do is press the button!  

I find the whole setting the kiln and working out Tempratures really difficult, my brain does not work well with numbers (unless its CASH!!) and it goes into melt down if I have to change settings..sad but true and nervewracking if I am experimenting with glass or colours!  But I think the Bead Cube is lovely and simple!

So my advice is hit that button and go for it!!

Good Luck
Jenniex
Title: Re: Annealing Bubbles
Post by: Kalorlo on June 17, 2010, 06:42:26 PM
I agree with Jennie! My BeadCube arrived today - I did a test run with it empty first, and made sure I could follow what the controller was saying and did things like stopping one program and starting the other when I noticed I'd begun with the batch one and it really wasn't necessary to have it heat up that slowly when it was empty...

Now it's batch annealing a biiiig pile of beads  :)