Title: Bead Sizing Tool!
Post by: Lush! on June 16, 2010, 10:33:06 AM
I'm sure somebody asked about how to get consistent bead sizes recently, I can't find the thread, but I did just come across this handy little tool on Etsy!

http://www.etsy.com/listing/49542680/smaller-lampwork-bead-sizers-for-bead?ref=v1_other_2
Title: Re: Bead Sizing Tool!
Post by: Redhotsal on June 16, 2010, 10:47:24 AM
Good Lord.
Title: Re: Bead Sizing Tool!
Post by: Diane on June 16, 2010, 11:13:47 AM
What will they think of next :o.  If they don't work you could always use them for blowing bubbles ;D
Title: Re: Bead Sizing Tool!
Post by: garishglobes on June 16, 2010, 11:16:20 AM
It looks like that game we used to have as kids - try to get the hoop over the bead without setting the alarm off!
Title: Re: Bead Sizing Tool!
Post by: fionaess on June 16, 2010, 12:25:50 PM
and dare I say it, what a very easy tool to make at home :) :) :)
Title: Re: Bead Sizing Tool!
Post by: poledra1958 on June 16, 2010, 12:35:53 PM
Quote from: fionaess on June 16, 2010, 12:25:50 PM
and dare I say it, what a very easy tool to make at home :) :) :)

Was thinking that myself

Jenny
Title: Re: Bead Sizing Tool!
Post by: sea-thistle on June 16, 2010, 12:40:27 PM
Yes I think you could easily make one yourself!! ::)
Title: Re: Bead Sizing Tool!
Post by: flaming beads on June 16, 2010, 12:49:09 PM
Genious idea though!..thanks julie ;D
Title: Re: Bead Sizing Tool!
Post by: dinah46 on June 16, 2010, 03:02:12 PM
Things to do with bent mandrels maybe :D
Title: Re: Bead Sizing Tool!
Post by: flaming beads on June 16, 2010, 03:04:03 PM
Lol...i've just gone through some of my bent mandrels, and decided to start using the other end :)